Rutting is one of the most important distresses in asphalt pavements due to its frequency. Rutting or channeling, could be classified in three types: 1) mechanical deformation (rutting in subgrade or base), 2) plastic flow (unstable asphalt layer), and 3) wheel path consolidation. The plastic flow of bituminous mixture depends on many factors; one of this is the type of asphalt used in the mixt...
To solve the problem of rutting and fatigue damage to asphalt pavement, rutting and fatigue performances of Qingchuan rock asphalt modified asphalt were studied, based on the dynamic shear rheometer test, the dynamic creep test, the rutting test, the indirect tensile fatigue test, the small-sized acceleration loading test, the compressive resilient modulus test, the BISAR3.0 Program and the rut...
BACKGROUND Quantifying vigilance and exploring the underlying mechanisms has been the subject of numerous studies. Less attention has focused on the complex interplay between contributing factors such as reproductive status, social rank, sex and group size. Reproductive status and social rank are of particular interest due to their association with mating behavior. Mating activities in rutting ...
rutting in asphalt concrete is a very common form of distress in asphalt concrete pavement which unfortunately has been incurable to date. one of the prime reasons of rutting is attributed to the behaviour of asphalt binder at elevated temperature. this study has investigated the performance of polypropylene fibres modified asphalt concrete mix against rutting. two types of asphalt concrete sam...
Rutting of flexible pavement is considered one of the major pavement distresses noted around the world and in Egypt. Many investigators showed at about 55 to 80% of rutting occurred in the surface layer. Rutting of asphalt surface layer may be due to many causes happened during construction phase and service phase. The main objectives of this research are to evaluate the impact of aggregate gra...
Construction of flexible pavements with hot mix asphalt (HMA) mixtures consumes huge energy which impacts the resources and the environment of the world. Warm Mix Asphalt (WMA) is an effective alternative as they produced with lower mixing and compaction temperature than those used in HMA production. This technology decreases energy consumption, saves money, and reducing the environmental pollu...
The three major distress conditions affecting the performance of asphalt pavements are permanent deformation or rutting, fatigue or load associated cracking, and low temperature or thermal cracking. In an earlier technical topics article (Fall, 1998), we examined the causes of fatigue cracking and the importance of good compaction during construction to help minimize this type of distress. In t...
Modifying asphalt binder with styrene butadiene rubber (SBR) improves low temperature performance (resistance to cracking), elastic recovery, and ductility of binder. However, some difficulties were found at high temperatures susceptibility (Rutting), storage stability (compatibility). Therefore, the aim this study is resolve these defects (rutting compatibility) by formulating SBR/ waste nanoc...