nanoindentation techniques are widely used for the study of nanomechanical properties of thin nanocomposite coatings. theoretical concepts and practical use of nanoindentation method are summarized with reporting the applications of these tests in characterization of some particular thin nanocomposite hybrid coatings prepared by sol-gel process. the better mechanical properties can be obtained ...
Hydrogels pose unique challenges to nanoindentation including sample preparation, control of experimental parameters, and limitations imposed by mechanical testing instruments and data analysis originally intended for harder materials. The artifacts that occur during nanoindentation of hydrated samples have been described, but the material properties obtained from hydrated nanoindentation have ...
Nanoindentation techniques are widely used for the study of nanomechanical properties of thin nanocomposite coatings. Theoretical concepts and practical use of nanoindentation method are summarized with reporting the applications of these tests in characterization of some particular thin nanocomposite hybrid coatings prepared by sol-gel process. The better mechanical properties can be obtained ...
Nanoindentation has become a standard method for measuring mechanical properties of bone, especially within microstructural units such as individual osteons or trabeculae. The use of nanoindentation to measure elastic properties has been thoroughly studied and validated. However, it is also possible to assess time dependent properties of bone by nanoindentation. The goal of this study was to co...
This study investigates polyacrylamide (PA) gel as a calibration material to measure the nanomechanical compressive modulus of cartilage using nanoindentation. Both nanoindentation and unconfined compression testing were performed on PA gel and porcine rib cartilage. The equilibrium moduli measured by the two methods were discernable. Nanoindentation has the advantage of distinguishing between ...
Introduction: Human cortical bone has been demonstrated as an anisotropic material. It has been shown that nanoindentation can be used to quantitatively reveal the anisotropy of cortical bone with the fact that different indentation modulus could be obtained at different indentation directions [1]. However, since nanoindentation analysis is developed based on isotropic material properties, test...
The accuracy of mechanical properties from depth-sensing indentation, or nanoindentation, depends on the accuracy of the displacement measurement used to calculate these properties. Here, current nanoindentation techniques and analysis methods for accurate displacement measurements are reviewed. First, the ability of a commercial instrument to sense the surface of soft materials is examined. Se...
Nanoindentation is used to determine the dynamic viscoelastic properties of six polymer materials. It is shown that varying the harmonic frequency of the nanoindentation does not have any significant effect on the measured storage and loss moduli of the polymers. Agreement is found between these results and data from DMA testing of the same materials. Varying the harmonic amplitude of the nanoi...
The hardness and elastic modulus of the cellulose fiber and polypropylene (PP) matrix in a cellulose fiber-reinforced PP composite were investigated by nanoindentation with a continuous stiffness technique. Nanoindentation with different indentation depths and spacings was conducted to measure hardness and elastic modulus in the interphase region, which was modified by maleic anhydride-grafted ...
Nanoindentation techniques are widely used for the study of nanomechanical properties of thin nanocomposite coatings. Theoretical concepts and practical use of nanoindentation method are summarized with reporting the applications of these tests in characterization of some particular thin nanocomposite hybrid coatings prepared by sol-gel process. The better mechanical properties can be obtained ...