نتایج جستجو برای: nanoindentation
تعداد نتایج: 2668 فیلتر نتایج به سال:
Elasto-plastic mechanical deformation behaviors of c-plane (0001) and nonpolar GaN single crystals are studied using nanoindentation, cathodoluminescence, and transmission electron microscopy. Nanoindentation tests show that c-plane GaN is less susceptible to plastic deformation and has higher hardness and Young's modulus than the nonpolar GaN. Cathodoluminescence and transmission electron micr...
TiN films were prepared by the Cathodic arc evaporation deposition method under different negative substrate bias. AFM image analyses show that the growth mode of biased coatings changes from 3D island to lateral when the negative bias potential is increased. Nanohardness of the thin films was measured by nanoindentation, and residual stress was determined using Grazing incidence X ray diffract...
In this study, mechanically alloyed Al 2024 powder is densified by conventional sintering and by equal channel angular pressing (ECAP) with and without back pressure. The powder was encapsulated in an aluminium can for consolidation through ECAP. The properties obtained in the compacts by conventional sintering route and by ECAP are compared. The effect of conventional sintering and ECAP on con...
We have demonstrated the utility of nanoindentation as a rapid characterization tool for mapping shape memory alloy compositions in combinatorial thin-film libraries. Nanoindentation was performed on Ni–Mn–Al ternary composition spreads. The indentation hardness and the reduced elastic modulus were mapped across a large fraction of the ternary phase diagram. The large shape memory alloy composi...
This review article is written on the investigations of nanomechanical properties of coatings by using nanoindentation techniques. The focus is on the studies that were conducted on epoxy polymer, silicones and their hybrid materials. The article describes a large number of developmental studies that are conducted on coatings. Materials properties such as nanoindentation hardness, modulus, scra...
Modern nanoindentation devices are capable of dynamic experimentations, which allow us to exploit instrumented hardness tests extensively. Beside the assets of recording mechanical properties continuously over displacement, there are ongoing debates whether the superimposed force alters the material's hardness. We will show for a broad range of materials that significant hardness differences ar...
Mechanical properties of the orthorhombic phase of YBa2Cu3O7-δ (Y-123) at room temperature have been investigated at different applied loads using nanoindentation technique. The study was carried out for several monodomains on the (001) planes for textured Bridgman samples with dispersed Y2BaCuO5 (Y-211) particles as pinning centers. The yield strength (σys), shear stress (τm) and toughness (KI...
The nanoindentation process of hydrated nacre has been simulated using threedimensional finite element method. The constitutive relation is based on Barthelat et al’s (Journal of the Mechanics and Physics of Solids, 2007, 55: 306-337) test results. The influence of the maximal loading on the simulation process is taken into account. The nanoindentation process and hardness of nacre are compared...
Famotidine Form B P. P. Upadhyay, M. K. Mishra, U. Ramamurty, A. D. Bond University of Copenhagen, Indian Institute of Science, University of Cambridge Purpose Polymorphs are well known to have different mechanical properties. Nanoindentation enables mechanical properties to be tested on single crystals, which should provide the best opportunity to establish a correlation with single-crystal X-...
Technical issues surrounding the use of nanoindentation at elevated temperatures are discussed, including heat management, thermal equilibration, instrumental drift, and temperature-induced changes to the shape and properties of the indenter tip. After characterizing and managing these complexities, quantitative mechanical property measurements are performed on a specimen of standard fused sili...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید