Jun Zheng Hui Zhou Binhua Gui Quanshun Luo Haixu Li Qimin Wang

In this study, AlCrN coatings were deposited using modulated pulsed power magnetron sputtering (MPPMS) with different power pulse parameters by varying modulated pulsed power (MPP) charge voltages (350 to 550 V). The influence of power pulse parameters on the microstructure, mechanical properties and thermal stability of the coatings was investigated. The results indicated that all the AlCrN co...

2010
Martin Moser Daniel Kiener Christina Scheu Paul H. Mayrhofer

Ti1-xAlxN coated tools are commonly used in high-speed machining, where the cutting edge of an end-mill or insert is exposed to temperatures up to 1100 °C. Here, we investigate the effect of Yttrium addition on the thermal stability of Ti1-xAlxN coatings. Reactive DC magnetron sputtering of powder metallurgically prepared Ti0.50Al0.50, Ti0.49Al0.49Y0.02, and Ti0.46Al0.46Y0.08 targets result in ...

2007
Travis Patterson

Modern gas turbine hot sections need to be protected from elevated temperature and damaging environments. This protection starts as a typically two layer coating system, the base layer or bond coat (BC) acts as a corrosion barrier and a kind of buffer for the thermal mismatch between the base material and the second top thermally protective layer or Thermal Barrier Coating (TBC). The BC is norm...

2017
Maryana Zagula-Yavorska Jan Sieniawski

A 0.5 μm thick layer of rhodium was deposited on the CMSX 4 superalloy by the electroplating method. The rhodium-coated superalloy was hafnized and aluminized or only aluminized using the Chemical vapour deposition method. A comparison was made of the microstructure, phase composition, and oxidation resistance of three aluminide coatings: nonmodified (a), rhodium-modified (b), and rhodiumand ha...

2005
G. Ovejero J. L. Sotelo M. D. Romero A. Rodríguez C. Diaz M. Corrias P. Kalck J. Garcia H. T. Gomes P. Serp F. L. Figueiredo F. L. Faria

The high external surface area leads to a significant increase in the surface contact between the gaseous or liquid reactants and the active phase supported on this nanostructured host which is a prerequisite for its use as catalyst support, especially in liquid phase medium where diffusion rate is predominant [2]. Also, the strong interactions between the exposed prismatic planes and the depos...

2015
Tobias V. Pfeiffer Puneet Kedia Maria E. Messing Mario Valvo Andreas Schmidt-Ott

This article introduces a continuous, gas-phase method for depositing thin metallic coatings onto (nano)particles using a type of physical vapor deposition (PVD) at ambient pressure and temperature. An aerosol of core particles is mixed with a metal vapor cloud formed by spark ablation by passing the aerosol through the spark zone using a hollow electrode configuration. The mixing process rapid...

Journal: :ChemElectroChem 2022

Abstract A nickel ferrite was prepared by a liquid‐phase method and used as an oxygen evolution catalyst in anion exchange membrane electrolyser. complete physicochemical characterization of the performed through X‐ray diffraction (XRD), Transmission electron microscopy (TEM) photoelectron spectroscopy (XPS). Then, deposited spray coating technique onto Fumasep® FAA3‐50 anion‐exchange to realiz...

Journal: :علوم و تکنولوژی پلیمر 0
علی طالبی محمدتقی خراسانی حمید میرزاده

in this study, porous scaffolds from poly(d,l-lactic acid) have been prepared via liquid- liquid phase separation method in ternary system of polymer-1,4-dioxane-water. polymer dissolved in dioxane in 1.5, 2.5 and 5 % wt/v and the solvent/non-solvent ratios were 13/87, 15/85 and 17/83. cloud point curves prepared by visual turbidometry. in order to obtain porous scaffolds with inter-connected p...

2018
Guo-Bin Sano Hideaki Uchiyama Guo-Bin Zheng Hideaki Sano Yasuo Uchiyama

A carbon nanotube-enhanced SiC (CNT-SiC) coating was deposited on C/C composites to improve the oxidation resistance of C/C. The CNT-SiC coating was prepared by direct growth of CNTs on C/C surface at 700oC followed by deposition of SiC using chemical vapor deposition at 1150oC for 1 hour. SiC was deposited on the CNTs as well as the interface between CNTs and C/C, making CNTs strongly rooted o...