Nian Xian Zhang Nguyen Q. Chinh Megumi Kawasaki Yi. Huang Terence G. Langdon Yi Huang

A Pb-62% Sn two-phase eutectic alloy was processed by high-pressure torsion (HPT) and stored at room temperature (RT) to investigate the occurrence of self-annealing. The microstructural characteristics and mechanical properties were recorded during self-annealing using scanning electron microscopy, tensile testing and nanoindentation. Processing by HPT produces a weakening effect but storage a...

2015
Eyup Cinar Ferat Sahin Dalia Yablon

A novel instrumentation approach to nanoindentation is described that exhibits improved resolution and depth sensing. The approach is based on a multi-probe scanning probe microscopy (SPM) tool that utilizes tuning-fork based probes for both indentation and depth sensing. Unlike nanoindentation experiments performed with conventional AFM systems using beam-bounce technology, this technique inco...

2012
Kangmin Xu Seung-Cheol Yang Xiaoping Qian

We present an approach for producing complex nanoscale patterns by integrating computer-aided design (CAD) geometry processing with an atomic force microscope (AFM) based nanoindentation process. Surface modification is achieved by successive nano-indentation using a vibrating tip. By incorporating CAD geometry, this approach provides enhanced design and patterning capability for producing geom...

2009
A. F. Gerday M. Ben Bettaieb L. Duchêne H. Diarra

Abstract: This paper focuses on the numerical modeling of nanoindentation tests. The first goal of this study is to collect essential material parameters and boundary conditions from the literature and to complete the data required to accurately model nanoindentation tests. The second goal of this study consists in validating the material parameters identified from macroscopic tensile tests of ...

2006
Y. Xiang X. Chen

We report on the results of a comparative study in which the mechanical response of both fully dense and porous lowdielectric thin films was evaluated using two different techniques: nanoindentation and the plane-strain bulge test. Stiffness values measured by nanoindentation are systematically higher than those obtained using the bulge test technique. The difference between the measurements is...

Journal: :CoRR 2016
Salah U. Hamim

Nanoindentation involves probing a hard diamond tip into a material, where the load and the displacement experienced by the tip is recorded continuously. This load-displacement data is a direct function of material's innate stress-strain behavior. Thus, theoretically it is possible to extract mechanical properties of a material through nanoindentation. However, due to various nonlinearities ass...

2015
Tommaso Nardi Chad Hammerquist John A. Nairn Ayat Karimi Jan-Anders E. Månson Yves Leterrier

Citation: Nardi T, Hammerquist C, Nairn JA, Karimi A, Månson J-AE and Leterrier Y (2015) Nanoindentation of functionally graded polymer nanocomposites: assessment of the strengthening parameters through experiments and modeling. Front. Mater. 2:57. doi: 10.3389/fmats.2015.00057 Nanoindentation of functionally graded polymer nanocomposites: assessment of the strengthening parameters through expe...

2008
J. Sort N. Van Steenberge S. Suriñach J. Eckert

The mechanical properties of a Zr55Cu30Al10Ni5 metallic glass rod are investigated by Vickers microhardness and depth-sensing nanoindentation. The alloy exhibits a relatively large hardness which decreases when increasing the maximum applied load. Serrated flow is also observed during nanoindentation. Both effects are related to deformationinduced mechanical softening.

Journal: :Materials Today 2013

Journal: :journal of ultrafine grained and nanostructured materials 2014
ahmad keyvani mohsen saremi mahmoud heydarzadeh sohi

conventional and nanostructured ysz coatings were deposited on the in-738 ni super alloy by the atmospheric plasma spray technique. the oxidation was measured at 1100°c in an atmospheric electrical furnace. according to the experimental results the nanostructured coatings showed a better oxidation resistance than the conventional ones. the improved oxidation resistance of the nanocoating could ...