Liang Song Erjun Guo Liping Wang Dongrong Liu Hugo F. Lopez

The effects of silicon (Si) on the mechanical properties and fracture toughness of heavy-section ductile cast iron were investigated to develop material for spent-nuclear-fuel containers. Two castings with different Si contents of 1.78 wt.% and 2.74 wt.% were prepared. Four positions in the castings from the edge to the center, with different solidification cooling rates, were chosen for micros...

2014
Sara C. Schvartzman Miguel A. Otaduy

This paper provides implementation details of the algorithm proposed in Schvartzman and Otaduy [2014] to simulate brittle fracture. We cast brittle fracture as the computation of a high-dimensional centroidal Voronoi diagram (CVD), where the distribution of fracture fragments is guided by the deformation field of the fractured object. We accelerate the fracture animation process with example-ba...

Abdollahzadeh, A., Shokuhfar, A.,

In this study, friction stir butt welding of Mg and Al alloys with applying Zn interlayer was performed. To obtain optimum condition, a combination of two travel and three rotation speeds were selected. Mg-Zn and Mg-Al-Zn IMCs, Al solid solution and residual Zn, were the most common phases in the stirred zone, which eliminated the formation of Al-Mg intermetallics. The maximum mechanical proper...

2017
Chao Gao Guorong Wu Sheng Wang

Results and Conclusions: The results show that, brittle fracture is the dominant way for SiC ceramic’s removal mechanism, plastic deformation always exists during the drilling process. Brittle fracture includes cleavage fracture, transgranular fracture, intergranular fracture, material peeling off and grain boundary breakage; resintering and recrystallization happen under the joint action of gr...

Journal: :Physical review letters 2015
Alessandro Lucantonio Giovanni Noselli Xavier Trepat Antonio DeSimone Marino Arroyo

Brittle materials propagate opening cracks under tension. When stress increases beyond a critical magnitude, then quasistatic crack propagation becomes unstable. In the presence of several precracks, a brittle material always propagates only the weakest crack, leading to catastrophic failure. Here, we show that all these features of brittle fracture are fundamentally modified when the material ...

Journal: :نشریه دانشکده فنی 0
علی عماری الهیاری حسن فرهنگی سید محمد مهدی هادوی

the effects of isothermal aging at temperatures between 550-850 ?c for durations of 1-100 h on microstructure, tensile properties, and impact fracture behavior of 316l austenitic stainless steel weld metal have been investigated. for this purpose, various techniques including metallographic observations, measurement of ferrite content using ferritscope, and fractographic investigations have bee...

Journal: :Physical review letters 2010
Clara B Picallo Juan M López Stefano Zapperi Mikko J Alava

We introduce a lattice model able to describe damage and yielding in heterogeneous materials ranging from brittle to ductile ones. Ductile fracture surfaces, obtained when the system breaks once the strain is completely localized, are shown to correspond to minimum energy surfaces. The similarity of the resulting fracture paths to the limits of brittle fracture or minimum energy surfaces is qua...

1998
M. L. Falk

A molecular-dynamics study of ductile and brittle fracture in model noncrystalline solids Abstract Molecular-dynamics simulations of fracture in model amorphous solids are shown to exhibit brittle or ductile behavior depending on small changes in interatomic potential. Yet, simulations of these two model solids under pure shear reveal no significant difference in their ultimate yield stress. To...

2012
Hao Wu Shreyes N. Melkote Steven Danyluk George W. Woodruff

This paper investigates the effect of crystallographic orientation on the mode of material removal (ductile vs. brittle) in diamond scribing of single crystal silicon (c-Si) and offers an explanation for the observed effects in terms of the combined role of phase transformation and slip generation. Single-point diamond scribing tests are performed on (111), (001) and (110) crystallographic plan...

2004
Shu Liu Yuh J. Chao Xiankui Zhu

The propensity of the transition of fracture type in either brittle or ductile cracked solid under mixed-mode I and III loading conditions is investigated. A fracture criterion based on the competition of the maximum normal stress and maximum shear stress is utilized. The prediction of the fracture type is determined by comparing smax=rmax at a critical distance from the crack tip to the materi...