نتایج جستجو برای: mode i fracture toughness
تعداد نتایج: 1335321 فیلتر نتایج به سال:
The fracture behaviour of human cortical bone was analysed considering a miniaturized version of the Double Cantilever Beam (DCB) test. A specific data reduction scheme based on crack equivalent concept was used to obtain the resistance curves. The definition of the cohesive laws mimicking the fracture process was performed measuring the crack tip opening displacement by digital image correlati...
Nowadays, laminated composites are widely used in the aerospace sector. All laminates have interply/interlaminar interfaces even if they made using automated processes. The act as areas of weaknesses and potential crack initiation regions. Hence, any enhancement propagation resistance is always sought after. Usage polymeric thin films one promising viable ways to achieve this. It also easy inco...
The effect of crack insertion for FDM printed PLA materials on Mode I and Mode II fracture toughness
In this investigation ‚the fracture toughness of A356 containing15%SiC composite was studied. Al/SiC composites have been considered because of their mechanical and erosion properties .Low fracture toughness in Al/SiC as compared with Aluminium alloys is one of its disadvantage. In this study at first A356 alloy was melted in a smelting electrical furnace then poured into the mould. A356-15% Si...
The objective of the work was to investigate statistical analysis of fracture toughness of the glass fiber reinforced composites at different stacking sequences, strain rate and crack length. The glass reinforced vinylester composites prepared by hand layup technique with stacking sequences of 0/90, 45/-45 and chopped strand orientations. 3point bending for fracture toughness test for various n...
The effects of silicon (Si) on the mechanical properties and fracture toughness of heavy-section ductile cast iron were investigated to develop material for spent-nuclear-fuel containers. Two castings with different Si contents of 1.78 wt.% and 2.74 wt.% were prepared. Four positions in the castings from the edge to the center, with different solidification cooling rates, were chosen for micros...
In this paper, using the Taguchi method, the parameters affecting the toughness of super duplex stainless steels in friction stir welding were optimized. In order to achieve optimal conditions, maximum toughness, the quality characteristic was used as the higher the better. Analysis of Taguchi results showed that in order to achieve optimal conditions in super duplex stainless steel weldments m...
Adhesive joints are continuously emerging as candidate to replace traditional fastening systems, such as riveting or welding, in primary structural applications. A wide class of components belonging to electronic, automotive and aerospace industries contains adhesive joints, however, the reliability during service constitutes a major technical problem as these contain flaws. Therefore, their us...
Cordierite was adhered to molybdenum using various metallic interlayers of copper, nickel, and chromium. The development of a coating adhesion test methodology was required to choose between interface designs. An indentation method was chosen because of ease in testing and availability of fracture mechanics interpretations of test data. The interfacial fracture toughness was determined from ind...