The fracture of carbon nanotubes is studied by atomistic simulations. In these simulations, the fracture behavior is found to be almost independent of the separation energy and to depend primarily on the inflection point in the interatomic potential. The results show moderate dependence of fracture strength on chirality. The range of fracture strains compares well with experimental results, but...
While hydrogen embrittlement of ferritic steels has been a subject of significant research, one of the major challenges in tackling hydrogen embrittlement is that the mechanism of embrittlement is not fully resolved. This paper reports new observations and interpretation of fracture surface features and deformation microstructures underneath the fracture surface, providing a mechanistic view of...
the dynamic behavior of three high manganese steels with very different stacking faultenergy (sfe) values (4-30 mj/m2) were studied using high strain rate torsional tests. the hotrolledmicrostructure of the steel with the lowest sfe of 4 mj/m2 consisted of a duplex mixture ofaustenite and ε-martensite, but those of the other two steels were fully austenitic. the deformedmicrostructures were stu...
dissimilar metals friction welding of austenitic–martensitic stainless steels is commonly used in order to manufacture engine valves in the automobile industry. in this study, x53crmnnin219 (austenitic stainless steel) and x45crsi93 (martensitic stainless steel) valve steel rods were welded by friction welding process. the welded joint was then heat treated at 760 0c for 60 min. mechanical prop...
Addition of titanium (Ti) to ASTM A710 Grade B Cu-precipitation-strengthened steel significantly increases the impact absorbed fracture energy and reduces the ductile-to-brittle transition temperature. The effect of Ti correlates with the reduction of the amount of pearlite in the ferritic microstructure. A thorough study of the mechanical properties of Ti-modified A 710B steel is presented. In...
Some forensic in situ investigations, such as those needed in transportation (for aviation, maritime, road, or rail accidents) or for parts working under harsh conditions (e.g., pipes or turbines) would benefit from a method/technique that distinguishes ductile from brittle fractures of metals—as material defects are one of the potential causes of incidents. Nowadays, the gold standard in mater...
Advanced ceramics and semiconductors (i.e. SiC, Si, Quartz, etc.) are increasingly being used for industrial applications. These ceramics/semiconductors are hard, strong, inert, and light weight. This combination of properties makes them ideal candidates for tribological, semiconductor, MEMS and optoelectronic applications. Manufacturing these materials without causing surface and subsurface da...