Introduction: The aim of this study was to evaluate the influenceof different light curing systems and curing times on the micro-hardness of aresin modified glass ionomer. Methods: Forty two samples of ResinModified Glass Ionomer (RMGI) were prepared using stainless steel cylindrical mold(8 × 2 mm) and randomly divided into six groups of seven. Three groups werecured with a Quartz Tungsten Halogen (QTH) light cure unit and the other threegroups were polymerized with LED unit for 20, 30 and 40 seconds. All sampleswere stored in distilled water for 24 hours. The micro-hardness was measured onthe top and bottom surfaces of the samples by Vickers hardness tester. Datawere analyzed by two–way ANOVA and Tukey’s post-hoc tests. Results: Two-wayANOVA showed that QTH light-cure unit had higher percentage in depth of curethan LED light-curing unit in both surfaces; whereas, the application time hasno significant effect on it. There was no interaction between two variables. Inboth light-curing groups, the values of top and bottom surfaces micro-hardnesswere increased as the application time increased, but there was not anystatistically significant difference among these groups except for 40-second groupof LED light-curing unit which was significantly higher than 20-second and30-second groups (P
منابع مشابه
the effects of exposure times and light curing sources on surface micro-hardness of a resin modified glass ionomer
introduction: the aim of this study was to evaluate the influenceof different light curing systems and curing times on the micro-hardness of aresin modified glass ionomer. methods: forty two samples of resinmodified glass ionomer (rmgi) were prepared using stainless steel cylindrical mold(8 × 2 mm) and randomly divided into six groups of seven. three groups werecured with a quartz tungsten halo...
متن کاملEffect of Light Curing Unit on Resin-modified Glass-ionomer Cements: a Microhardness Assessment
OBJECTIVE To evaluate the microhardness of resin-modified glass-ionomer cements (RMGICs) photoactivated with a blue light-emitting diode (LED) curing light. MATERIAL AND METHODS Thirty specimens were distributed in 3 groups: Fuji II LC Improved/GC (RM1), Vitremer/3M ESPE (RM2) and Filtek Z250/3M ESPE (RM3). Two commercial light-curing units were used to polymerize the materials: LED/Ultrablue...
متن کاملSurface hardness properties of resin-modified glass ionomer cements and polyacid-modified composite resins.
In this study the top and bottom surface hardness of two polyacid-modified composite resins (PMCRs), one resin-modified glass ionomer cement (RMGIC), and one composite resin were evaluated. The affect of water storage on their hardness was also investigated. The study was conducted using four different groups, each having five specimens obtained from fiberglass die molds with a diameter of 5 mm...
متن کاملComparative Evaluation of Surface Hardness of Different Resin-Modified Glass Ionomers and a Compomer
Introdouction: Due to the practical problems and time restriction issues in treating dental problems in children, there is a noticeable demand for the application of a convenient handling restorative material with acceptable physical-mechanical properties. The aim of this investigation was to evaluate Vickers microhardness of four tooth-colored restorative materials as a determining mechanical...
متن کاملEffect of etching and light-curing time on the shear bond strength of a resin-modified glass ionomer cement.
The aim of this study was to assess the influence of etching and light-curing time on the shear bond strength (SBS) and adhesive remnant index (ARI) of a resin-modified glass ionomer cement (RMGIC) upon debonding of orthodontic brackets. Sixty-eight bovine permanent incisors were obtained and embedded in acrylic resin. Edgewise metallic brackets were bonded to the teeth with Fuji Ortho LC RMGIC...
متن کاملHardness of composite resin polymerized with different light-curing units
Introduction: The degree of polymerization depends on the type of light-curing unit. The aim of this study was to compare the hardness of composite resin cured by LED and Halogen light curing units. Methods: In this experimental study, 20 cylindrical samples of Tetric Ceram composite were prepared. Half of them were cured with Ultralume 2 LED and the other half with Astralis 7 Halogen light ...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 3 شماره 2
صفحات 77- 81
تاریخ انتشار 2014-06-01
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
کلمات کلیدی
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023