Shear Bond Strength of Metal brackets to Zirconia Treated with Er:YAG Laser Sandblasting and Silane
نویسندگان
چکیده مقاله:
Background and Aim: Application of zirconia ceramics has increased. Since the commonly used surface treatment for porcelain, i.e. acid etching is not efficient for zirconia surfaces, evaluation of other surface treatment methods for zirconia is important. The aim of this study was to compare the shear bond strength (SBS) of metal brackets to zirconia treated with different powers of Er:YAG laser, sandblasting and silane. Materials and Methods: In this experimental study, five blocks of 3 mol% yttria stabilized tetragonal zirconia ceramics (3Y-TZP-A) were cut into small cubes. After the sintering process, 72 samples were assigned to six groups (n=12). The first group did not receive any surface treatment. The second, third and fourth groups were irradiated with Er:YAG laser with 1.5 W (150 mJ), 2.5 W (250 mJ) and 3 W (300 mJ) powers, respectively in a long pulse mode for 20 seconds. The samples in the fifth group were sandblasted. The sixth group samples were silanized. After bonding of brackets to the samples, they were stored in distilled water, thermocycled and their SBS was measured by a universal testing machine. Mode of failure was assessed by a stereomicroscope. Results: The SBS of brackets to zirconia in groups one to six was 0.31±0.23, 0.51±0.14, 1.11 ±0.40, 3.32±1.52, 9.5±2.99 and 3.88±2.20 MPa, respectively. ANOVA revealed a significant difference among the six groups. Tamhane’s test showed that the SBS in group five was significantly higher than that in the other groups. Bond failure occurred at the adhesive/zirconia interface in all groups. Conclusion: Surface treatment of zirconia with sandblasting provided appropriate bond strength of brackets for clinical applications. But, Er:YAG laser and silane did not create sufficient SBS to zirconia surfaces.
منابع مشابه
A Comparative Evaluation of Shear Bond Strength of Creation Ceramic Veneer to Metal and Zirconia Cores
Abstract Background and Aim: High chipping rates of the veneering porcelain of zirconia ceramic restorations have been reported in clinical studies. Thus, the shear bond strength (SBS) between the zirconia core and veneering porcelain requires investigation. Materials and Methods: In this in-vitro study, at first, using a computer-aided design/computer-aided manufacturing (CAD/CAM) machine, 1...
متن کاملShear bond strength between resin and zirconia with two different silane blends.
OBJECTIVE To study in vitro the effect of two cross-linking silanes, bis-1,2-(triethoxysilyl)ethane and bis[3-(trimethoxysilyl)propyl]amine, blended with an organofunctional silane coupling agent, (3-acryloxypropyl)trimethoxysilane, on the shear bond strength between resin-composite cement and silicatized zirconia after dry storage and thermocycling. MATERIALS AND METHODS Six tested groups of...
متن کاملEvaluation of the Effect of Sandblasting (120 μm) on Shear Bond Strength between Ceramic Veneer and Zirconia Core
Background and Aim: Due to the importance of the bond strength between zirconia core (ZC) and porcelain veneer (PV) as well as the paradox about the functionality of sandblasting on the solidity between those layers, this research aimed to evaluate the effect of sandblasting on the shear bond strength (SBS) between ZC and PV. Materials and Methods: After preparing 20 zirconia discs (7 mm &time...
متن کاملShear Bond Strength of Nanocomposites to Dentin Substrate Treated with Er:YAG Laser Followed by Two Different Bonding Systems
Background and Aim: Preparation of tooth structure by laser systems produces a surface with different characteristics. Therefore, selecting an appropriate bonding system is necessary to achieve the maximum bond strength. The aim of this study was to compare the bond strength of Adper Single Bond 2 adhesive and Single Bond Univer-sal to dentin prepared by bur or laser. Materials and Methods: ...
متن کاملEffects of femtosecond laser and other surface treatments on the bond strength of metallic and ceramic orthodontic brackets to zirconia
Femtosecond laser has been proposed as a method for conditioning zirconia surfaces to boost bond strength. However, metallic or ceramic bracket bonding to femtosecond laser-treated zirconia surfaces has not been tested. This study compared the effects of four conditioning techniques, including femtosecond laser irradiation, on shear bond strength (SBS) of metallic and ceramic brackets to zircon...
متن کاملShear bond strength of self-ligating brackets.
The aim of this study was to compare the shear bond strength (SBS) and adhesive remnant index (ARI) scores of conventional and self-ligating brackets. Conventional stainless steel brackets (group 1, Step; Leone) and three different passive and interactive self-ligating brackets (group 2, Smart Clip, 3M Unitek; group 3, Quick, Forestadent; and group 4, Damon 3MX, Ormco) were tested. Four groups ...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 28 شماره 3
صفحات 110- 117
تاریخ انتشار 2016-07
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023