Friction stir welding (FSW) is a promising technique to join aluminum alloys without having problems encountered during fusion welding processes. In the present work, the evolution of microstructure and texture in friction stir welded thin AA2024 aluminum alloy are examined by electron backscattered diffraction (EBSD) technique. The sheets with 0.8 mm thickness were successfully welded by friction stir welding at the tool rotational speeds of 500, 750, and 1000 rpm with a constant traverse speed of 160 mm/min. EBSD revealed that stir zones exhibited equiaxed recrystallized grains and the grain size increased with increasing the tool rotation rate. The fraction of high angle grain boundaries and mean misorientation angle of the boundaries in the FSW joints at 500 rpm were 63.6% and 24.96°, respectively, which were higher than those of the sample welded at 1000 rpm (53.6% and 17.37°). Crystallographic texture results indicated that the Cube {001}<100> and S {123}<634> textures in base metal gradually transformed in to Copper {112}<111> shear texture. It was found that with increasing the tool rotation rate, the intensity of Cube {001}<100>, Y {111}<112>, S {123}<634>, and Dillamore {4 4 11}<11 11 8> texture orientations increased and the intensity of Brass {011}<211> texture orientation decreased.
منابع مشابه
Tensile properties and fracture locations of friction-stir-welded joints of 2017-T351 aluminum alloy
Friction stir welding (FSW) is a new and promising welding process that can produce low-cost and high-quality joints of heat-treatable aluminum alloys because it does not need consumable filler materials and can eliminate some welding defects such as crack and porosity. In order to demonstrate the friction stir weldability of the 2017-T351 aluminum alloy and determine optimum welding parameters...
متن کاملThe Microstructure and Mechanical Properties of Friction Stir Welded Ti6al4v Titanium Alloy under Β Transus Temperature
1 Faculty of Aerospace Engineering, Shenyang Aerospace University, No. 37 Daoyi South Avenue, Daoyi Development District, Shenyang 110136, China 2 State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology, No. 92 West Dazhi street, Nangang District, Harbin 100024, China 3 Beijing Aeronautical Manufacturing Technology Research Institute, No. 1 Dongjun Village, Chaoyang...
متن کاملMicrostructure Evolution and Shaping of Friction Stir Lap Welded Dissimilar Magnesium Alloy Joint
Friction stir lap welding (FSLW) experiment has been conducted on 3mm thick AZ80 extruded sheet and 2.3mm thick AZ31B rolled sheet. The influence of the shape of the taper thread mixing head on microstructure has been discussed. Pores forming, hooked defects, interface migration, tissue distribution have been analyzed. The organization of both sides of nugget zone (NZ) is arranged diagonally ab...
متن کاملDevelopment of mathematical model to predict the mechanical properties of friction stir welded AA6351 aluminum alloy
This paper presents a systematic approach to develop the mathematical model for predicting the ultimate tensile strength, yield strength, and percentage of elongation of AA6351 aluminum alloy which is widely used in automotive, aircraft and defense Industries by incorporating (FSW) friction stir welding process parameter such as tool rotational speed, welding speed, and axial force. FSW has bee...
متن کاملEffect of Post-weld Heat Treatment on Joint Properties of Dissimilar Friction Stir Welded AA2024 and AA7075 Aluminum Alloys
In present study, the effect of heat treatment after friction stir welding dissimilar welds T6-7075 and T4-2024 aluminum alloys were investigated. Friction stir welding was performed at a constant rotation speed of 1140 rpm and welding speed 32 mm/min. After welding samples are taken under various heat treatment processes at different aging temperature and time period. Microstructural observati...
متن کاملFatigue of Friction Stir Welded 2024-T351 Aluminium Alloy
Fatigue failure characteristics of friction stir welds in 13mm gauge 2024-T351 plate have been assessed. Failure occurred from either the weld region (nugget/flow arm) or from the material immediately surrounding the weld. Fatigue failure from the surrounding material was essentially conventional, initiating from large S-phase intermetallic particles and growing in a macroscopic mode I manner. ...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 15 شماره 1
صفحات 53- 63
تاریخ انتشار 2018-03
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023