Influence of 10-MDP Adhesive System on Shear Bond Strength of Zirconia-Composite Interfaces

نویسندگان

  • Meike Stiesch Department of Prosthetic Dentistry and Biomedical Materials Research, Hannover Medical School, Carl-Neuberg-Str. 1, 30625 Hannover, Germany
  • Michael Eisenburger Department of Prosthetic Dentistry and Biomedical Materials Research, Hannover Medical School, Carl-Neuberg-Str. 1, 30625 Hannover, Germany
  • Philipp Cornelius Pott Department of Prosthetic Dentistry and Biomedical Materials Research, Hannover Medical School, Carl-Neuberg-Str. 1, 30625 Hannover, Germany
چکیده مقاله:

  Introduction: This in-vitro study investigated the initial 24h bond strength between different composites and zirconia after application of four different adhesive systems. Methods: A total of 120 specimens of zirconia (InCoris, Sirona, Germany, Bernsheim) were ground with a 165 µm grit rotating diamond disc. Thirty specimens were each additionally treated with Cimara Zircon “CZ” (VOCO GmbH, Germany, Cuxhaven), Futurabond U “FBU” (VOCO GmbH), Futurabond M+ “FBM” (VOCO GmbH) or Futurabond M+ in combination with the DCA activator “FBMD” (VOCO GmbH). One of three different types of composites – BifixSE (“BS”), BifixQM (“BQ”) or GrandioSO (“G”) (VOCO GmbH) – was bonded to ten specimens each in every group. Shear bond strength (SBS) was determined in a universal testing machine. Statistical analysis was performed with ANOVA and the Tukey test. Results: FBM and FBMD gave higher SBS than CZ and FBU in combination with all tested composites. In comparison to FBU, FBM gave statistically significant increases in SBS with BifixSE (19.4±5.7 MPa) (P

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Influence of artificial aging on the shear bond strength of zirconia-composite interfaces after pretreatment with new 10-MDP adhesive systems

Introduction: This in-vitro study investigates the bond strength of different zirconia composites  with three different modern adhesive systems after artificial aging using thermocycling and water storage. Methods: A total of 90 specimens of zirconia (InCoris, Sirona, Germany, Bernsheim) were ground using a 165 µm grit rotating diamond disc. Thirty specimens were additionally treated with eithe...

متن کامل

Influence of artificial aging on the shear bond strength of zirconia- composite interfaces after pretreatment with new 10-MDP adhesive systems

Introduction: This in-vitro study investigates the bond strength of different zirconia composites with three different modern adhesive systems after artificial aging using thermocycling and water storage. Methods: A total of 90 specimens of zirconia (InCoris, Sirona, Germany, Bernsheim) were ground using a 165 μm grit rotating diamond disc. Thirty specimens were additionally treated with either...

متن کامل

Micro-Raman Vibrational Identification of 10-MDP Bond to Zirconia and Shear Bond Strength Analysis

So far, there is no report regarding the micro-Raman vibrational fingerprint of the bonds between 10-methacryloyloxy-decyl dihydrogen phosphate (10-MDP) and zirconia ceramics. Thus, the aim of this study was to identify the Raman vibrational peaks related to the bonds of 10-MDP with zirconia, as well as the influence on microshear bond strength. Micro-Raman spectroscopy was employed to assess t...

متن کامل

Shear bond strength of indirect composite material to monolithic zirconia

PURPOSE This study aimed to evaluate the effect of surface treatments on bond strength of indirect composite material (Tescera Indirect Composite System) to monolithic zirconia (inCoris TZI). MATERIALS AND METHODS Partially stabilized monolithic zirconia blocks were cut into with 2.0 mm thickness. Sintered zirconia specimens were divided into different surface treatment groups: no treatment (...

متن کامل

The influence of rotating fatigue on the bond strength of zirconia-composite interfaces.

OBJECTIVES To evaluate the effect of cyclic loading on the bond strength of resin composite to zirconia framework material. METHODS Bar shaped zirconia/composite specimens (2 mm x 2 mm x 25 mm) were prepared using three different resin cements and placed in a four-point bending test setup. The flexure strength (F(s)) was calculated by placing the bars (n=10) fixed between the four supports (a...

متن کامل

Shear bond strength of Composite / Amalgam restorations: Effect of using adhesive cement

Shear bond strength of Composite / Amalgam restorations: Effect of using adhesive cement Dr. M. Khoroushi *- Dr. M. Yeganehjo ** *Assistant Professor of Operative Dentistry & Dental Materials Dept., Faculty of Dentistry, Isfahan University of Medical Sciences. ** Dentist. Abstract Background and Aim: The aim of this study was to evaluate the shear bond strength (SBS) of composite/amalgam restor...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 4  شماره 3

صفحات  117- 126

تاریخ انتشار 2015-09-01

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023