Objective: Corrosion resistance is among the most important properties of metal alloys used in the oral cavity. Consumption of acidic foods reduces the salivary pH and intensifies the corrosion of brackets and orthodontic wires. This study aimed to compare electro galvanic corrosion of different orthodontic brackets and wires and determine the amount of ions released into acidic artificial saliva. Methods: In this in vitro experimental study, 24 mandibular incisor brackets of 4 different manufacturers (Dentaurum, American Orthodontics, Shinye and ORJ) with stainless steel (SS) or nickel-titanium (Ni-Ti) round wires 0.016 were immersed in acidic artificial saliva for 28 days and their potential difference with the reference electrode was recorded. The amount of released ions was measured in the solution using atomic absorption method. Data were analyzed using two-way ANOVA and repeated measures ANOVA. Results: The mean amount of ions released was not significantly different between groups (p>0.05). The potential difference of Shinye brackets coupled to SS wire was significantly lower than that of other combinations and was negative throughout the study. The potential difference of Dentaurum bracket-NiTi wire, ORJ bracket-NiTi wire, Shinye bracket-SS wire and ORJ bracket-SS wire combinations at the end of experiment was negative as well. Conclusion: The galvanic corrosion of Shinye bracket coupled to SS wire in acidic artificial saliva was greater than that of other bracket-wire combinations. The specimens were not significantly different in terms of the released ions.
Download for Free
Sign up for free to access the full text
Sign up - It's Free!اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودمنابع مشابه
galvanic corrosion and ion release from different orthodontic brackets and wires in acidic artificial saliva: part i
objective: corrosion resistance is among the most important properties of metal alloys used in the oral cavity. consumption of acidic foods reduces the salivary ph and intensifies the corrosion of brackets and orthodontic wires. this study aimed to compare electro galvanic corrosion of different orthodontic brackets and wires and determine the amount of ions released into acidic artificial sali...
متن کاملGalvanic Corrosion of Orthodontic Brackets and Wires in Acidic Artificial Saliva: Part II
Objective: Orthodontic wires should have high resistance against corrosion in the oral environment. Since the effect of pH on corrosion has been well recognized, this study sought to assess and compare the electrochemical corrosion of orthodontic brackets and wires of different brands in acidic artificial saliva. Methods: This in vitro experimental study was conducted on 24 mandibular centr...
متن کاملgalvanic corrosion of orthodontic brackets and wires in acidic artificial saliva: part ii
objective: orthodontic wires should have high resistance against corrosion in the oral environment. since the effect of ph on corrosion has been well recognized, this study sought to assess and compare the electrochemical corrosion of orthodontic brackets and wires of different brands in acidic artificial saliva. methods: this in vitro experimental study was conducted on 24 mandibular central...
متن کاملGalvanic corrosion between orthodontic wires and brackets in fluoride mouthwashes.
The aim of this investigation was to determine the influence of fluoride in certain mouthwashes on the risk of corrosion through galvanic coupling of orthodontic wires and brackets. Two titanium alloy wires, nickel-titanium (NiTi) and copper-nickel-titanium (CuNiTi), and the three most commonly used brackets, titanium (Ti), iron-chromium-nickel (FeCrNi) and cobalt-chromium (CoCr), were tested i...
متن کاملGalvanic Corrosion of and Ion Release from Various Orthodontic Brackets and Wires in a Fluoride-containing Mouthwash.
Background and aims. This study compared the galvanic corrosion of orthodontic wires and brackets from various manufacturers following exposure to a fluoride mouthwash. Materials and methods. This study was conducted on 24 lower central incisor 0.022" Roth brackets of four different commercially available brands (Dentaurum, American Orthodontics, ORJ, Shinye). These brackets along with stainles...
متن کاملGalvanic Corrosion among Different Combination of Orthodontic Archwires and Stainless Steel Brackets
Introduction: The aim of this study was to assess the galvanic behavior of different bracket and archwire combinations that are commonly used in orthodontic treatments. Methods: Three types of orthodontic archwires with a diameter of 0.016×0.022 inch and 80 standard edgewise maxillary central incisor brackets were selected. Three groups consisted of different wire-bracket couples and one group ...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 32 شماره None
صفحات 37- 44
تاریخ انتشار 2014-02
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023