Evaluation of the Effect of Sandblasting (120 μm) on Shear Bond Strength between Ceramic Veneer and Zirconia Core

نویسندگان

  • D Ghalebaaghi
  • GR Esfahani Zadeh , Prosthodontics Dept, Dental Branch of Tehran, Islamic Azad University, Tehran, Iran
  • M Noor Bakhsh Assistant Professor, Prosthodontics Dept, Dental Branch of Tehran, Islamic Azad University, Tehran, Iran
  • MH Salari Assistant Professor, Prosthodontics Dept, Dental Branch of Tehran, Islamic Azad University, Tehran, Iran
چکیده مقاله:

Background and Aim: Due to the importance of the bond strength between zirconia core (ZC) and porcelain veneer (PV) as well as the paradox about the functionality of sandblasting on the solidity between those layers, this research aimed to evaluate the effect of sandblasting on the shear bond strength (SBS) between ZC and PV. Materials and Methods: After preparing 20 zirconia discs (7 mm × 3 mm) in this experimental study, they were randomly divided into two groups of case and control. In the case group, sandblasting with 120-μm aluminum oxide particles (Al2O3) was performed under 3.5-bar pressure at 10 mm distance from the zirconia surface for 15 seconds. Next, all the samples were cleaned with ultrasonic and 96% isopropyl alcohol for 3 minutes as well as steam cleaning for 10 seconds. Then, the samples were veneered with porcelain (3 mm × 5 mm). SBS was assessed using a universal testing machine. After data collection, the mean and standard deviation (SD) were calculated and analyzed using T-test. Results: The SBS between ZC and PV was 62.56±8.35 MPa in the case group (after sandblasting) and 94.62±7.69 MPa in the control group. The SBS showed a significant statistical difference between the two groups (P=0.001). Conclusion: The result of this research indicated that sandblasting reduces the SBS between ZC and PV. Considering the limitations and the methodology of the study, the hypothesis regarding the positive impact of sandblasting on SBS was not proven.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

A Comparative Evaluation of Shear Bond Strength of Creation Ceramic Veneer to Metal and Zirconia Cores

Abstract Background and Aim: High chipping rates of the veneering porcelain of zirconia ceramic restorations have been reported in clinical studies. Thus, the shear bond strength (SBS) between the zirconia core and veneering porcelain requires investigation. Materials and Methods: In this in-vitro study, at first, using a computer-aided design/computer-aided manufacturing (CAD/CAM) machine, 1...

متن کامل

Shear Bond Strength of Metal brackets to Zirconia Treated with Er:YAG Laser Sandblasting and Silane

Background and Aim: Application of zirconia ceramics has increased. Since the commonly used surface treatment for porcelain, i.e. acid etching is not efficient for zirconia surfaces, evaluation of other surface treatment methods for zirconia is important. The aim of this study was to compare the shear bond strength (SBS) of metal brackets to zirconia treated with different powers of Er:YAG lase...

متن کامل

The effect of multiple firings on microtensile bond strength of core-veneer zirconia-based all-ceramic restorations.

PURPOSE Differences in core and veneer coefficients of thermal expansion, firing shrinkage, and speed of increasing and decreasing the temperature may generate stress in veneered all-ceramic restorations. Given the necessity of performing multiple firing cycles to achieve improved contour, color, and esthetics, the purpose of this study was to determine the effect of multiple firing cycles on t...

متن کامل

The effect of various sandblasting conditions on surface changes of dental zirconia and shear bond strength between zirconia core and indirect composite resin

PURPOSE To measure the surface loss of dental restorative zirconia and the short-term bond strength between an indirect composite resin (ICR) and zirconia ceramic after various sandblasting processes. MATERIALS AND METHODS Three hundred zirconia bars were randomly divided into 25 groups according to the type of sandblasting performed with pressures of 0.1, 0.2, 0.4 and 0.6 MPa, sandblasting t...

متن کامل

Evaluation of shear bond strength between dual cure resin cement and zirconia ceramic after thermocycling treatment

PURPOSE This study was performed to evaluate shear bond strength (SBS) between three dual-cured resin cements and silica coated zirconia, before and after thermocycling treatment. MATERIALS AND METHODS Sixty specimens were cut in 15 × 2.75 mm discs using zirconia. After air blasting of 50 µm alumina, samples were prepared by tribochemical silica coating with Rocatec™ plus. The specimens were ...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 3  شماره 2

صفحات  31- 36