Effect of Post-weld Heat Treatment on Joint Properties of Dissimilar Friction Stir Welded AA2024 and AA7075 Aluminum Alloys

نویسندگان

  • Safarbali, B. Department of Materials Engineering, Isfahan University of Technology, Isfahan, Iran
  • Eslami, A. Department of Materials Engineering, Isfahan University of Technology, Isfahan, Iran
  • Shamanian, M. Department of Materials Engineering, Isfahan University of Technology, Isfahan, Iran
چکیده مقاله:

In present study, the effect of heat treatment after friction stir welding dissimilar welds T6-7075 and T4-2024 aluminum alloys were investigated. Friction stir welding was performed at a constant rotation speed of 1140 rpm and welding speed 32 mm/min. After welding samples are taken under various heat treatment processes at different aging temperature and time period. Microstructural observations, phase analysis characterization and mechanical properties were performed on welded before and after heat treatment in cross section of welds joint. The results showed that post-weld heat treatment causes abnormal grain growth turns destructive effect on the mechanical properties, while formation of fine and uniform precipitation recovery strength and ductility of welds joints. It is found heat treatment based on T6-7075 and T6-2024 procedure has highest and lowest impact on the restore of weld strength. Tensile test indicate that fracture occurred on the interface between TMAZ and HAZ in retreating side (7075) at as-weld joint, if that failure happens in the stir zone by applying PWHT. Surface fracture suggested fractures in PWHT samples are predominantly inter-granular, while in as-weld joint the fractures of joints are mostly trans-granular.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of tool position on microstructural and mechanical properties of friction stir butt welded joint of AA2024–AA7075 dissimilar alloys

In this research, butt joining of Al2024 and Al7075 plates were performed by Friction Stir Welding (FSW) and the effect of tool position on microstructural and mechanical properties in about 1 mm from center line of joint towards the advancing side (AS) and the retreating side (RS) was investigated at three positions of +1, 0, -1 mm. In this regard, the plates of Al2024 and Al7075 were selected...

متن کامل

Effect of Heat Input on Tensile Properties of Friction Stir Welded AA6061-T6 and AA7075-T6 Dissimilar Aluminum Alloy Joints

Friction Stir Welding (FSW) is a solid state process widely used to join dissimilar aluminium alloys. High quality and strength joints can be fabricated using this technique when compared to other conventional methods. The welding parameters play major role in determining the quality of the weld. This paper aims in presenting the effect of heat input on tensile properties of the joints between ...

متن کامل

Liquation Cracking of Dissimilar Aluminum Alloys during Friction Stir Welding

A liquation cracking mechanism of dissimilar Al alloys during the friction stir welding (FSW) is suggested in this study. To identify the mechanism, the precipitates were analyzed and Al-Mg-Cu phase diagrams were calculated. Electron backscattering diffraction (EBSD) analysis and electron probe microanalysis (EPMA) were also conducted. In the same manner as constitutional liquation, at high hea...

متن کامل

Effect of nanoparticles addition on dissimilar joining of aluminum alloys by friction stir welding

The purpose of this study was to examine the effect of adding Nano particles such as Nano Carbon Tube during Friction Stir Welding (FSW) on dissimilar Al alloy joints. More specifically, both FSW and Friction Stir Processing (FSP) were performed simultaneously to investigate the effect of adding Nano particles on mechanical properties and microstructure of the weld zone for joining AA5754-H22 a...

متن کامل

Effect of heat treatment on the grain structure and mechanical properties of Al-7075 friction stir weld

The fine grain structure of friction-stir welded aluminum alloys is unstable during post weld heat treatment and some grains abnormally grown. In this study, the sequence of abnormal grain growth during T6 heat treatment of Al-7075 friction-stir weld and its effect on mechanical properties of the weld was studied. The results showed that heat treatment in 510 ˚C resulted in drastic grain growth...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 5  شماره 1

صفحات  1- 11

تاریخ انتشار 2019-09

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

کلمات کلیدی

کلمات کلیدی برای این مقاله ارائه نشده است

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023