Sodium fluoride addition to a two-step etch-and-rinse adhesive system: effect on dentin microtensile bond strength and durability

Authors

  • Homayoun Alaghehmand ,Dental Materials Research Center, Health Research Institute, Babol University of Medical Sciences,Babol, IR Iran.
  • Soraya Khafri ,Infertility and Reproductive Health Research Center, Health Research Institute, Babol University of Medical Sciences, Babol, IR Iran.
  • Yasaman Samani ,Student Research Committee, Babol University of Medical Sciences,Babol, IR Iran.
  • Zahra Jafari ,Department of Operative Dentistry, Faculty of Dentistry, Mazandaran University of Medical Sciences,Sari, IR Iran.
Abstract:

Introduction: Studies have suggested that sodium fluoride (NaF) has an inhibitory effect on the activity of endogenous matrix metalloproteinase enzymes. This study assessed the effect of a fluoride-containing adhesive on microtensile bond&nbsp;strength (&micro;TBS) over time. Material & Methods: In this experimental study, 36 extracted &nbsp;third molars were used to evaluate the &micro;TBS of a 5th generation adhesive modified by NaF. The exposed dentin surfaces were abraded and built up using composite resin. Then, the specimens were randomly divided into three groups of 12 teeth based on the type of adhesive used: Solobond M with no inhibitor (control); Solobond M with 5,000 ppm NaF; and Solobond M with 10,000 ppm NaF. The &micro;TBS and failure mode of specimens were evaluated after 24-hour and 3-month storage in distilled water. Data were analyzed using ANOVA and Tukey&rsquo;s test. P<0.05 was considered as significant level. Results: The control group demonstrated a lower &micro;TBS than the experimental groups after 24 hours and 3 months (p<0.05). The &micro;TBS was higher in adhesive with 5,000 ppm NaF than in control group after 3 months (p<0.05). The group with 10,000 ppm NaF had the highest &micro;TBS after 24 hours and 3 months (p<0.05). Conclusion: The fluoride-containing adhesives showed significantly higher bond strength values than the original adhesive without fluoride after 24-hour and 3-month storage in distilled water, leading to the improvement of resin-dentin bonds.

Upgrade to premium to download articles

Sign up to access the full text

Already have an account?login

similar resources

Effect of water storage on microtensile bond strength of a two-step self-etch adhesive and a two-step etch-and-rinse adhesive.

This study evaluated the effect of 24 h (1d) and one-year (1yr) water storage on the microtensile dentin bond strength of a two-step total-etch and a two-step self-etch adhesive system. Ten extracted human third molars were sectioned perpendicularly to their long axis to expose flat occlusal dentin surfaces. Teeth were divided into two groups (n=5) according to the adhesive used: a two-step etc...

full text

Strength and Durability of a New Adhesive Bond to Superficial Dentin Using Etch and Rinse and Self-Etch Systems: An In Vitro Study

Background and Aim: Data regarding the efficacy of universal adhesives are limited. This study aimed to assess the durability of a universal adhesive bond to superficial dentin using etch and rinse and self-etch modes. Materials and Methods: In this in vitro, experimental study, 32 sound molars were randomly divided into two groups of Scotchbond Universal adhesive with two-step etch and rins...

full text

Effect of Tannic Acid Application on Durability of Bond of Etch and Rinse Adhesive Resins

Aim: To determine the effect of different concentrations and application times of tannic acid on bond strength to dentin. Materials and Methods: Occlusal surfaces of 180 human molars were randomly divided into two groups of immediate shear bond strength evaluation and evaluation after 2 months of storage in collagenase solution. Each group was divided into 10 subgroups according to the solution...

full text

Effect of Solvent Type on Microtensile Bond Strength of a Total-etch One-bottle Adhesive System to Moist, Dry Dentin

This study evaluated the effect of organic solvent (acetone or ethanol) on the microtensile bond strengths (MTBS) of an adhesive system applied to dry and moist dentin. Sixteen extracted human third molars were ground to expose a flat occlusal dentin surface and acid etched for 20 seconds (20% phosphoric acid gel, Gluma Etch 20 Gel, Heraeus/Kulzer). After rinsing the acid etchant, an ethanol-ba...

full text

Bond Strength of Total-Etch Dentin Adhesive Systems on Peripheral and Central Dentinal Tissue: A Microtensile Bond Strength Test

Objective: The purpose of this study was to evaluate the microtensile bond strength (μ TBS) of four total-etch adhesives [Excite (EB), Prime & Bond NT (PBNT), Single Bond (SB), and One Coat Bond (OCB)] by comparing them to five self-etching adhesives (Clearfil SE Bond (CSEB), Xeno III (X III), Prompt L-Pop (PLP), AQ Bond (AQB), and Tyrian/One Step plus (TOSP)] at different dentinal areas. In ad...

full text

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 7  issue None

pages  16- 23

publication date 2018-09

By following a journal you will be notified via email when a new issue of this journal is published.

Keywords

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023