Abstract:

Formation of stray grain defects particularly around re-entrant features of the turbine blade airfoils is one of the major problems in directional and single crystal solidification processes. In this work, directional solidification tests of the GTD-111 Ni-based superalloy were conducted at different withdrawal velocities of 3, 6 and 9 mm.min-1 using various stepped cylindrical and cubic designs. The process was also simulated using ProCAST finite element solver to characterize the crystal orientations. The phase transformation temperatures of the superalloy were estimated by the differential scanning calorimetry test. A process map was developed to predict the formation of stray grains in the platform regions of the stepped cylindrical and cubic specimens using the experimentally-validated simulation model. The process map shows critical values of the platform size, withdrawal velocity and initial sample size for the stray grain formation. The withdrawal velocity, platform size and initial sample size all had an inverse effect on the formation of stray grains.

Download for Free

Sign up for free to access the full text

Already have an account?login

similar resources

A Thermomechanical Fatigue Crack Initiation Model for Directionally-solidified Ni-base Superalloys

Nickel-base superalloys have been used extensively in power generation applications due to their high strength at temperatures up to 1093°C. When the material is subjected to complex mechanical loading superimposed with thermal loading, fatigue interacts with either creep and/or oxidation. Directionallysolidified (DS) materials are often used in place of polycrystalline (PC) materials since the...

full text

Freckle Defect Formation near the Casting Interfaces of Directionally Solidified Superalloys

Freckle defects usually appear on the surface of castings and industrial ingots during the directional solidification process and most of them are located near the interface between the shell mold and superalloys. Ceramic cores create more interfaces in the directionally solidified (DS) and single crystal (SX) hollow turbine blades. In order to investigate the location of freckle occurrence in ...

full text

Thermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy

A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...

full text

Precipitation in a Ni - Al - Mo Directionally Solidified Eutectic Composite

The most recently developed high temperature materials are known as in-situ composites or directionally solidified eutectics. Since the composites are formed during solidification, they have excellent morphological stabilities up to near their melting temperatures. The Ni-Al-Mo system has received the greatest attention for recent several years(1)~(3) since the alloy is expected to form a struc...

full text

Effect of pre-exposure on crack initiation life of a directionally solidified Ni-base superalloy

Article history: Received 6 February 2008 Received in revised form 1 July 2008 Accepted 24 July 2008 Available online 5 August 2008

full text

On oscillatory microstructure during cellular growth of directionally solidified Sn–36at.%Ni peritectic alloy

An oscillatory microstructure has been observed during deep-cellular growth of directionally solidified Sn-36at.%Ni hyperperitectic alloy containing intermetallic compounds with narrow solubility range. This oscillatory microstructure with a dimension of tens of micrometers has been observed for the first time. The morphology of this wave-like oscillatory structure is similar to secondary dendr...

full text

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 14  issue 4

pages  12- 24

publication date 2017-12

By following a journal you will be notified via email when a new issue of this journal is published.

Keywords

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023