Investigation of Corrosion Behavior and Galvanic Corrosion Simulation of Super Duplex Stainless Steel UNS S32750 Weld Zone

Authors

  • Ahl Sarmadi, M. Isfahan University of Technology, Farsan Sanat Parsian Company
  • ,
  • Atapour, M. Isfahan University of Technology, Farsan Sanat Parsian Company
  • Behjat, A. Isfahan University of Technology, Farsan Sanat Parsian Company
  • Edriss, H. Isfahan University of Technology, Farsan Sanat Parsian Company
  • Vahman , M. Isfahan University of Technology, Farsan Sanat Parsian Company
Abstract:

Galvanic corrosion is an ever-present problem in all different environments, particularly in tanks. The goal of this project is to develop a finite element model that can be used with experimental data to characterize the corrosion of a galvanic weldments couple in an electrolyte. In this study sample are welded by gas tungsten arc welding and friction stir welding. According to ASTM G8, Evaluation of corrosion properties examined with cyclic polarization test in 0.5 molar H2SO4 andthe information required to validate the model was prepared. The finite element model is developed using COMSOL and Math Module through derivation of equations describing corrosion thermodynamics and electrochemical kinetics. The results showed that reducing in heat input to improve galvanic corrosion behavior in the weld sample.In addition to result of simulation reveal sample that welded by gas tungsten arc method had higher current density galvanic corrosion in comparison with friction stir sample.

Download for Free

Sign up for free to access the full text

Already have an account?login

similar resources

Evaluation of the corrosion behavior of the base metal and weld metal sections of the super duplex stainless steel UNS S32750

In this study, the corrosion behavior of super duplex stainless steel UNS S32750 and tungsten arc welding with filler metals AWS ER2594 duplex stainless steel in acidic solution containing chloride ions have been investigated. Microstructure of weld joints evaluateby light and electron microscope and corrosion behavior examine by open circuit potential and cyclic polarization tests.The results ...

full text

Evaluation of the corrosion behavior of the base metal and weld metal sections of the super duplex stainless steel UNS S32750

In this study, the corrosion behavior of super duplex stainless steel UNS S32750 and tungsten arc welding with filler metals AWS ER2594 duplex stainless steel in acidic solution containing chloride ions have been investigated. Microstructure of weld joints evaluateby light and electron microscope and corrosion behavior examine by open circuit potential and cyclic polarization tests.The results ...

full text

Corrosion Behavior of Stainless Steel Clad Rebar

Stainless steel clad rebar (SCR) was investigated because it may become a cost-effective means of controlling corrosion in concrete under very aggressive environments. Sound SCR (316L cladding) resisted corrosion in saturated Ca(OH)2 solution (SCS) with up to 5 wt% chloride. Cladding breaks on SCR induced significant corrosion of exposed underlying CS in SCS with only 1 wt% chloride. A computer...

full text

Influence of multiple welding cycles on microstructure and corrosion resistance of a super duplex stainless steel

.......................................................................................... v Appended Publications .................................................................. vii Table of

full text

جوشکاری فولاد زنگ ‌نزن سوپر دو فازی S32750 UNSبه‌روش اصطکاکی اغتشاشی و ارزیابی ریزساختار، خواص مکانیکی و خوردگی آن

Super duplex stainless steel is a kind of duplex stainless steel that has pitting resistant equivalent number over than 40. Unified Numbering System (UNS) S32750 is a common super duplex stainless stee, that is mostly applied in oil and gas refinery industries, because of its proper corrosion-resistant properties . Therefore, joining of these steels by welding is very important, but the greates...

full text

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 4  issue 1

pages  113- 126

publication date 2018-08

By following a journal you will be notified via email when a new issue of this journal is published.

Keywords

No Keywords

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023