HOT CRACK FORMATION IN PURE CU AND CU-30%ZN ALLOY DURING IN SITU SOLIDIFICATION
Authors
Abstract:
The hot cracking susceptibility can be determined by establishing the transition temperature between brittle and ductile fracture at high temperature tensile testing of in situ solidified samples. High temperature tensile properties were determined for commercial cathodic pure Cu and Cu- 30%Zn alloy. The transition temperatures for pure Cu and Cu-30%Zn were evaluated from ultimate tensile stress, true strain and area reduction at different testing temperatures. The results show that hot cracking in pure Cu also occurred below and near to its melting temperature. It can be proposed that in this case excess vacancies and vacancy diffusion and condensation are the dominating mechanisms for hot crack formation. The transition temperature for Cu- 30%Zn was much lower than its solidus temperature and this alloy has more susceptibility to hot cracking as compared to pure Cu. The effect of two different cooling rates (15 °C/min and 60 °C/min) on the transition temperature was investigated. The results show that by increasing cooling rate, the transition temperature will increase. The morphology of fracture surfaces for both ductile and brittle modes were evaluated by SEM Two different morphologies, i.e. interdendiritic and intergranual fracture, was found.
similar resources
' * , sy Solidification Behavior and Structure of AI - Cu Alloy Welds
The microsegregation behavior of electron beam (EB, and gas tungsten arc (GTA) welds of Al-Cu alloys covering a range from 0.19 to 7.74 wt% Cu were characterized for dendrite core concentrations and fraction eutectic solidification. Although a single weld speed of 12.7 mm/sec was used, some differences were observed in the segregation behavior of the two weld types. The microsegregation behavio...
full textsimulation and experimental studies for prediction mineral scale formation in oil field during mixing of injection and formation water
abstract: mineral scaling in oil and gas production equipment is one of the most important problem that occurs while water injection and it has been recognized to be a major operational problem. the incompatibility between injected and formation waters may result in inorganic scale precipitation in the equipment and reservoir and then reduction of oil production rate and water injection rate. ...
In Situ and Real-Time Observation of the Solidification Process of Al20mass%Cu Alloy by Synchrotron X-ray Radiography
High brilliance synchrotron X-ray radiography has been used to in situ study the solidification process of Al20mass%Cu alloy with nominal spatial and temporal resolutions of 7.4 μm and 300ms, respectively. The block of favorably oriented dendrites by the unfavorably oriented ones was first observed in metal solidification, which related to solute interaction of neighbor dendrites. Solute inter...
full textFormation, Thermal Stability and Mechanical Properties of Cu-Zr and Cu-Hf Binary Glassy Alloy Rods
Glassy alloy rods with diameters up to 1.5mm exhibiting a large supercooled liquid region before crystallization and high mechanical strength were formed in Cu-Zr and Cu-Hf binary alloy systems by the copper mold casting method. The large supercooled liquid region exceeding 40K was obtained in the composition range of 30 to 70 at%Zr and 35 to 60 at%Hf. The largest value of the supercooled liqui...
full textMicrostructural Evolution and Dynamic Softening Mechanisms of Al-Zn-Mg-Cu Alloy during Hot Compressive Deformation
The hot deformation behavior and microstructural evolution of an Al-Zn-Mg-Cu (7150) alloy was studied during hot compression at various temperatures (300 to 450 °C) and strain rates (0.001 to 10 s-1). A decline ratio map of flow stresses was proposed and divided into five deformation domains, in which the flow stress behavior was correlated with different microstructures and dynamic softening m...
full textTEXTURE AND RESISTIVITY OF Cu and DILUTE Cu ALLOY FILMS
Annealing of dilute binary Cu(Ti), Cu(In), Cu(Al), Cu(Sn), Cu(Mg), Cu(Nb), Cu(B), Cu(Co) and Cu(Ag) alloy films resulted in the strongest <111> fiber texture for Cu(Ti) and the lowest resistivity for Cu(Ag). The behavior of the alloy films was compared and contrasted with that for a pure evaporated Cu film. Electron beam evaporated films with compositions in the range of 2.0-4.2 at% and thickne...
full textMy Resources
Journal title
volume 3 issue 1
pages 9- 15
publication date 2006-06
By following a journal you will be notified via email when a new issue of this journal is published.
No Keywords
Hosted on Doprax cloud platform doprax.com
copyright © 2015-2023