Abstract:

Introduction: The aim of this study was to assess the galvanic behavior of different bracket and archwire combinations that are commonly used in orthodontic treatments. Methods: Three types of orthodontic archwires with a diameter of 0.016×0.022 inch and 80 standard edgewise maxillary central incisor brackets were selected. Three groups consisted of different wire-bracket couples and one group was just brackets as a control group. Each group had five samples. Four brackets were then connected to each wire by elastic bands made from electrochemically neutral material. The samples were immersed into capped containers of Fusayama-Meyer artificial saliva. After six weeks, the released nickel ions were quantified via ion absorption technique. The mean and the standard deviation of all four groups were calculated and the data were compared together with Kruskal-Wallis non-parametric statistical test. Results: The highest concentration of released nickel ions was for bracket+ steel archwire and the least for the bracket without archwire. Conclusion: There were not significant differences among experimental groups, so it could be concluded that galvanic corrosion would not be a serious consideration through orthodontic treatment.  

Download for Free

Sign up for free to access the full text

Already have an account?login

similar resources

galvanic corrosion among different combination of orthodontic archwires and stainless steel brackets

introduction: the aim of this study was to assess the galvanic behavior of different bracket and archwire combinations that are commonly used in orthodontic treatments. methods: three types of orthodontic archwires with a diameter of 0.016×0.022 inch and 80 standard edgewise maxillary central incisor brackets were selected. three groups consisted of different wire-bracket couples and one group ...

full text

Comparison of Mechanical Properties between Different Orthodontic Stainless Steel Archwires

Introduction: The Damon system recommended the use of revolutionary, hightechnology Damon edgewise 0.019” x 0.025” orthodontic stainless steel archwires (OSSA) for major mechanics and finishing and claimed that this new archwires offer greater efficiency during orthodontic treatment. No study has been carried out to compare this relatively new archwires to other popular OSSA already in the mark...

full text

Galvanic corrosion between orthodontic wires and brackets in fluoride mouthwashes.

The aim of this investigation was to determine the influence of fluoride in certain mouthwashes on the risk of corrosion through galvanic coupling of orthodontic wires and brackets. Two titanium alloy wires, nickel-titanium (NiTi) and copper-nickel-titanium (CuNiTi), and the three most commonly used brackets, titanium (Ti), iron-chromium-nickel (FeCrNi) and cobalt-chromium (CoCr), were tested i...

full text

Effect of acetic NaF solution on the corrosion behavior of stainless steel orthodontic brackets.

This study assessed the effect of acetic NaF solutions on stainless steel orthodontic brackets. Acetic acid was added to a 0.1% NaF solution to make two solutions, one with pH 3.5 and the other with pH 6. For the two different stainless steel brackets (Tomy, Dentaurum) used in this study, they had a similar elemental composition--except with Mo (molybdenum) in the Tomy bracket. The brackets wer...

full text

In -Vitro: Evaluation of Corrosion Behavior of Orthodontic Stainless Steel Brackets to Salad Dressing

The objectives of this study were to investigate the corrosion behavior of conventional and self-ligating stainless steel brackets and the surface structural changes in response to salad dressing. Damon, In-Ovation,Smart clip, Discovery, OMNI and Masel brackets were all included in the study. For the control group, the brackets were placed in Petri dishes with Potassium Ferrocyanide (Fe [CN]6K4...

full text

Galvanic Corrosion of Orthodontic Brackets and Wires in Acidic Artificial Saliva: Part II

  Objective: Orthodontic wires should have high resistance against corrosion in the oral environment. Since the effect of pH on corrosion has been well recognized, this study sought to assess and compare the electrochemical corrosion of orthodontic brackets and wires of different brands in acidic artificial saliva.   Methods: This in vitro experimental study was conducted on 24 mandibular centr...

full text

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 3  issue 3

pages  118- 122

publication date 2014-09-01

By following a journal you will be notified via email when a new issue of this journal is published.

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023