Solvent extraction of copper from the copper leach solution obtained from the ammoniacal carbonate leaching of the Sarcheshmeh copper concentrate was carried out, and the performance of CP-150, LIX984N, and Kelex100 as well as the effects of different parameters involved were investigated. According to the results obtained, the extraction kinetics of all the three extractants was fast. High concentrations (7.5%, V/V) of CP-150 and Kelex100 were required to completely extract copper, while only 1% of LIX984N was sufficient. Addition of hexane to the diluent decreased the capability of CP-150 to extract copper, while it showed less effects on LIX984N and Kelex100. A desirable stripping of copper from the loaded organic phase could be obtained using H2SO4 solution.
similar resources
Copper Recovery from Chalcopyrite Concentrate by an Indigenous Acidithiobacillus ferrooxidans in an Air-Lift Bioreactor
In this study, effects of solid concentration, temperature, and initial Fe2+ concentration on bioleaching of sulfide mineral (chalcopyrite) obtained from Sarcheshmeh Copper Mine in the region of Kerman located in the south of Iran were investigated. A mesophilic iron oxidizing bacterium, Acidithiobacillus ferrooxidans has been isolated from a typical chalcopyrite copper concentra...
full textComparison of Copper Dissolution in Chalcopyrite Concentrate Bioleaching with Acidianus Brierleyi in Different Initial pH Values
Although bioleaching of chalcopyrite by thermophilic microorganisms enhances the rate of copper recovery, a high temperature accelerates iron precipitation as jarosite, which can bring many operational problems in the industrial processes. In this research work, the bioleaching of chalcopyrite concentrate by the thermophilic Acidianus brierleyi was studied, and the microbial grow...
full textOptimization of parameters affecting recovery of copper from Sarcheshmeh low-grade sulfide ore using Bioleaching
In this work, the parameters affecting the recovery of copper from the low-grade sulfide minerals of Sarcheshmeh Copper Mine were studied. A low-grade sulfide ore was used with a copper grade of 0.25%, which was about 28% of the mineral oxide, and the sulfide minerals made up the rest. Much more sulfide minerals were found to be pyrite and most of the gangue minerals were quartz, anorthite, bio...
full textcopper recovery from chalcopyrite concentrate by an indigenous acidithiobacillus ferrooxidans in an air-lift bioreactor
in this study, effects of solid concentration, temperature, and initial fe2+ concentration on bioleaching of sulfide mineral (chalcopyrite) obtained from sarcheshmeh copper mine in the region of kerman located in the south of iran were investigated. a mesophilic iron oxidizing bacterium, acidithiobacillus ferrooxidans has been isolated from a typical chalcopyrite copper concentrate of the menti...
full textcomparison of zoe and vitapex for canal treatment of necrotic primary teeth
چکیده ندارد.
15 صفحه اولRecovery of Copper from Copper Slag and Copper Slag Flotation Tailings by Oxidative Leaching
Copper smelter slag and copper smelter slag flotation tailings were leached using sulphuric acid solutions, without or with the addition of either ferric sulphate or hydrogen peroxide. Copper extraction from the slag was typically found to be twice as high as that from the slag flotation tailings. Hydrogen peroxide was determined to be the best lixiviant. Thus, copper and iron extractions were ...
full textMy Resources
Journal title
volume 9 issue 2
pages 393- 402
publication date 2018-04-01
By following a journal you will be notified via email when a new issue of this journal is published.
Hosted on Doprax cloud platform doprax.com
copyright © 2015-2023