Compaction of Commercially Pure Titanium Powder by Friction Powder Compaction Process
نویسندگان
چکیده
A new friction powder compaction (FPC) process is introduced for compacting commercially pure titanium powder. The FPC process is very simple and energy-efficient since it requires only a rotating tool plunged into an aluminum plate with a hole filled with titanium powder, and no external heat source is necessary. The sintering of the powder is mainly achieved by the friction heat and pressing load generated by the rotating tool in the aluminum plate and powder. The microstructure and Vickers hardness of the compacted titanium powder were investigated. It was shown that titanium powder was satisfactorily compacted by the FPC process. [doi:10.2320/matertrans.MC201208]
منابع مشابه
Numerical Methods for Predicting Roll Press Powder Compaction Parameters
Large numbers of cohesive powders are compacted using a roll press. The principle of compaction is that particulate materials become a compact when they are subjected to high pressure. Experimental work was carried out on pharmaceutical powders [1] to determine the influence of operating parameters on the roll process compaction. Theses parameters are determined for a given powder and must be m...
متن کاملAn Arbitrary Lagrangian-eulerian Finite Element Method for Cone-cap Plasticity; Application to Powder Compaction Simulation
The compaction forming of metal powder is a process involving large deformations, large strain, non-linear material behavior and friction. Consequently, the numerical analysis of such a highly non-linear process is a formidable computational problem. In this paper, an ALE technique is presented based on a generalized cap plasticity model in simulation of powder forming processes. In ALE formula...
متن کاملEffects of compaction pressure and particle shape on the porosity and compression mechanical properties of sintered Ti6Al4V powder compacts for hard tissue implantation.
Sintered Ti6Al4V powder compacts potentially to be used in implant applications were prepared using commercially available spherical and angular powders (100-200 mum) within the porosity range of 34-54%. Cylindrical green powder compacts were cold compacted at various pressures and then sintered at 1200 degrees C for 2 h. The final percent porosity and mean pore sizes were determined as functio...
متن کاملWear and Friction Analysis of Sintered Metal Powder Self Lubricating Bush Bearing
Abstract—Powder metallurgy (P/M) is the only economic way to produce porous parts/products. P/M can produce near net shape parts hence reduces wastage of raw material and energy, avoids various machining operations. The most vital use of P/M is in production of metallic filters and self lubricating bush bearings and siding surfaces. The porosity of the part can be controlled by varying compacti...
متن کاملStudy of Compaction and Ejection Properties of Powder Mixes Processed by Warm Compaction
Warm compaction takes advantage of temperature to favor densification during compaction. However, this technique requires powder mixes with specific physical characteristics to be adequately processed in the temperature range involved in warm pressing. The mix formulation, especially the lubricant/binder system, should provide good flowability and compressibility and lubrication of the die wall...
متن کامل