Residual Tensile Property of Plain Woven Jute Fiber/Poly(Lactic Acid) Green Composites during Thermal Cycling
نویسندگان
چکیده
This study investigated the residual tensile properties of plain woven jute fiber reinforced poly(lactic acid) (PLA) during thermal cycling. Temperature ranges of thermal cycling tests were 35-45 °C and 35-55 °C. The maximum number of cycles was 10³ cycles. The quasi-static tensile tests of jute fiber, PLA, and composite were conducted after thermal cycling tests. Thermal mechanical analyses of jute fiber and PLA were conducted after thermal cycling tests. Results led to the following conclusions. For temperatures of 35-45 °C, tensile strength of composite at 10³ cycles decreased 10% compared to that of composite at 0 cycles. For temperatures of 35-55 °C, tensile strength and Young's modulus of composite at 10³ cycles decreased 15% and 10%, respectively, compared to that of composite at 0 cycles. Tensile properties and the coefficient of linear expansion of PLA and jute fiber remained almost unchanged after thermal cycling tests. From observation of a fracture surface, the length of fiber pull out in the fracture surface of composite at 10³ cycles was longer than that of composite at 0 cycles. Therefore, tensile properties of the composite during thermal cycling were decreased, probably because of the decrease of interfacial adhesion between the fiber and resin.
منابع مشابه
Creep Behavior of Poly(lactic acid) Based Biocomposites
Polymer composites containing natural fibers are receiving growing attention as possible alternatives for composites containing synthetic fibers. The use of biodegradable matrices obtained from renewable sources in replacement for synthetic ones is also increasing. However, only limited information is available about the creep behavior of the obtained composites. In this work, the tensile creep...
متن کاملEffect of Chemical Treatments on the Physical Properties of Non-woven Jute/PLA Biocomposites
Biocomposites based on poly(L-lactic acid) (PLA) and non-woven jute fabrics (NWJF) were fabricated by sandwiching non-woven jute mat between PLA sheets. First, composites were fabricated with various weight proportions of jute fabric (5, 10, 20, and 30 wt.%) with the PLA matrix, and the effect of fabric loading on their mechanical properties was investigated. Higher mechanical properties were f...
متن کاملTensile properties and damage evolution in vascular 3D woven glass/epoxy composites
Vascularization enables multifunctional composites capable of self-healing, thermal regulation, electrical and magnetic modulation, and damage sensing. In this study, the effect of vascular channels on the in-plane tensile properties and damage progression of three-dimensional orthogonally woven textile composites is examined. Vascular channels are manufactured by Vaporization of Sacrificial Co...
متن کاملCompletely biodegradable soyprotein–jute biocomposites developed using water without any chemicals as plasticizer
Soyprotein–jute fiber composites developed using water without any chemicals as the plasticizer show much better flexural and tensile properties than polypropylene–jute composites. Co-products of soybean processing such as soy oil, soyprotein concentrate and soy protein isolates are inexpensive, abundantly available and are renewable resources that have been extensively studied as potential mat...
متن کاملAccelerated Heat Aging Study of Phenolic/Basalt Fiber Reinforced Composites
One of the greatest impediments to use polymer-matrix composites is their susceptibility to degradation when exposed to the elevated temperatures and the limited knowledge on the thermal and mechanical properties of these composites at such temperatures. The objective of this study is to evaluate the effects of accelerated heat aging on the tensile properties of the Woven Basalt/Phenolic (WBP) ...
متن کامل