The repair of a fractured porcelain surface with a resin composite was investigated. The effects of applying an opaque resin to porcelain surfaces, which were silanated by a ceramic primer from a repair kit or by an experimental silane coupling agent, were studied. The porcelain surfaces were silanated for 10 sec and 60 min. Three types of adherents were evaluated: opaque resin with light irradiation (OWL), opaque resin without light irradiation (ONL), and no opaque resin (NAO). The shear bond strengths of the resins to the porcelain surfaces were measured before and after thermocycling. The maximum shear bond strength (6.7 MPa) after thermocycling was observed when the silanating period of the ceramic primer was 60 min. The opaque resin had no effect on the bond strength. Moreover, the bond strength obtained with the experimental silane coupling agent was found to be reduced by only 2 MPa, even after thermocycling.
منابع مشابه
مقایسه اثر سه ماده اچ کننده پرسلن (PHA-APF-HF) بر روی استحکام برشی باند کامپوزیت- پرسلن
Statement of Problem: Porcelain restorations are susceptible to fracture and a common method for repairing is the use of silane and composite on etched porcelain. Although HF is very effective in porcelain etching but has detrimental effects on tissues. Purpose: In this study, the effect of APF and PHA was compared with HF in porcelain etching. Also the role of silane, unfilled resin and dentin...
متن کاملShear strength of the composite bond to etched porcelain.
The shear bond strength of composite resin to porcelain was investigated to optimize variables for bonding porcelain laminate veneers. Scanning electron microscopy was initially used to examine the surface configuration of porcelain prepared under various conditions. A factorial experiment was undertaken to determine the effects of three different bonding methods on both etched and non-etched p...
متن کاملThe 24-year clinical performance of porcelain laminate veneer restorations bonded with a two-liquid silane primer and a tri-n-butylborane-initiated adhesive resin.
This report describes the bonding technique and clinical course of porcelain laminate veneer restorations applied to discolored maxillary incisors and canines. The patient was an 18-year-old woman, and tooth reduction was limited to the enamel. Laminate veneer restorations were made with a feldspathic porcelain material (Cosmotech Porcelain). After try-in, enamel surfaces were etched with 65% p...
متن کاملPreparing porcelain surfaces for optimal bonding.
When placing an indirect restoration such as a porcelain veneer, inlay, or onlay, the intaglio surface is typically treated in some fashion to ensure optimal bonding to the resin-based adhesives and luting cements required to affix it to the tooth tissues. A variety of surface preparation techniques have been advocated, including the use of acids, particle abrasion, various adhesives, and chemi...
متن کاملBonding of the silane containing multi-mode universal adhesive for lithium disilicate ceramics
OBJECTIVES This study evaluated the influence of a multi-mode universal adhesive (MUA) containing silane (Single Bond Universal, 3M EPSE) on the bonding of resin cement to lithium disilicate. MATERIALS AND METHODS Thirty IPS e.max CAD specimens (Ivoclar Vivadent) were fabricated. The surfaces were treated as follows: Group A, adhesive that did not contain silane (ANS, Porcelain Bonding Resin,...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Bio-medical materials and engineering
دوره 24 6 شماره
صفحات -
تاریخ انتشار 2014