Bond strength of direct and indirect bonded brackets after thermocycling.

نویسندگان

  • Jacob Daub
  • David W Berzins
  • Brandon James Linn
  • Thomas Gerard Bradley
چکیده

Thermocycling simulates the temperature dynamics in the oral environment. With direct bonding, thermocycling reduces the bond strength of orthodontic adhesives to tooth structure. The purpose of this study was to evaluate the shear bond strengths (SBS) of one direct and two indirect bonding methods/adhesives after thermocycling. Sixty human premolars were divided into three groups. Teeth in group 1 were bonded directly with Transbond XT. Teeth in group 2 were indirect bonded with Transbond XT/Sondhi Rapid Set, which is chemically cured. Teeth in group 3 were indirect bonded with Enlight LV/Orthosolo and light cured. Each sample was thermocycled between 5 degrees C and 55 degrees C for 500 cycles. Mean SBS in groups 1, 2, and 3 were not statistically significantly different (13.6 +/- 2.9, 12.3 +/- 3.0, and 11.6 +/- 3.2 MPa, respectively; P > .05). However, when these values were compared with the results of a previous study using the same protocol, but without thermocycling, the SBS was reduced significantly (P = .001). Weibull analysis further showed that group 3 had the lowest bonding survival rate at the minimum clinically acceptable bond-strength range. The Adhesive Remnant Index was also determined, and group 2 had a significantly (P < .05) higher percentage of bond failures at the resin/enamel interface.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Comparison of shear bond strength of stainless steel brackets bonded with three light- cured adhesives

Introduction: The bonding process of the brackets to enamel has been a critical issue in orthodontic research. The purpose of this study was to evaluate the shear bond strength of 3 light-cured adhesives (transbond XT, Z250, light bond). Materials &Methods: In this study sixty extracted human premolars were collected and randomly divided into 3 test groups. All teeth were etched by 37% phosp...

متن کامل

Comparing the Effect of Assure Plus and Transbond XT Bonding on Shear Bond Strength and Adhesive Remnant Index in Metal Brackets Bonded to Enamel

Background and purpose: Bracket debonding is a major problem during orthodontic treatment. This research aimed at studying shear bond strength (SBS) and adhesive remnant index (ARI) in two bonding systems (Assure Plus (adhesion booster) and control). Materials and methods: In this vitro trial, premolars (n=90) were divided into two groups. The brackets were bonded either with Transbond XT or A...

متن کامل

Shear Bond Strength of Metallic and Ceramic Brackets Bonded with Two-step and Three-step Light Cure Adhesives

  Background and purpose: The bonding process is highly important in orthodontic treatment for its fast speed. The purpose of this study was to compare the shear bond strength of ceramic and metallic brackets between three stage (transbondTM XT) and two stage (GC ortho connectTM) light cure composites. Materials and methods: In this experimental study, 80 maxillary and mandibular first and sec...

متن کامل

Comparison of shear bond strength of the stainless steel metallic brackets bonded by three bonding systems

Introduction: In orthodontic treatment, it is essential to establish a satisfactory bond between enamel and bracket. After the self-etch primers (SEPs) were introduced for the facilitation of bracket bonding in comparison to the conventional etch-and-bond system, multiple studies have been carried out on their shear bond strengths which have yielded different results. This study was aimed at co...

متن کامل

Effect of silica coating on bond strength between a gold alloy and metal bracket bonded with chemically cured resin

OBJECTIVE The purpose of this study was to evaluate the effects of three different surface conditioning methods on the shear bond strength (SBS) of metal brackets bonded directly to gold alloy with chemically cured resin. METHODS Two hundred ten type III gold alloy specimens were randomly divided into six groups according to the combination of three different surface conditioning methods (alu...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • The Angle orthodontist

دوره 76 2  شماره 

صفحات  -

تاریخ انتشار 2006