Electrochemical and mechanical behavior of laser processed Ti-6Al-4V surface in Ringer's physiological solution.

نویسندگان

  • Raghuvir Singh
  • S K Tiwari
  • Suman K Mishra
  • Narendra B Dahotre
چکیده

Laser surface modification of Ti-6Al-4V with an existing calcium phosphate coating has been conducted to enhance the surface properties. The electrochemical and mechanical behaviors of calcium phosphate deposited on a Ti-6Al-4V surface and remelted using a Nd:YAG laser at varying laser power densities (25-50 W/mm(2)) have been studied and the results are presented. The electrochemical properties of the modified surfaces in Ringer's physiological solution were evaluated by employing both potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) methods. The potentiodynamic polarizations showed an increase in the passive current density of Ti-6Al-4V after laser modification at power densities up to 35 W/mm(2), after which it exhibited a decrease. A reduction in the passive current density (by more than an order) was observed with an increase in the laser power density from 25 to 50 W/mm(2). EIS studies at the open circuit potential (OCP) and in the passive region at 1.19 V showed that the polarization resistance increased from 8.274 × 10(3) to 4.38 × 10(5) Ω cm(2) with increasing laser power densities. However, the magnitudes remain lower than that of the untreated Ti-6Al-4V at OCP. The average hardness and modulus of the laser treated Ti-6Al-4V, evaluated by the nanoindentation method, were determined to be 5.4-6.5 GPa (with scatter <±0.976 GPa) and 124-155 GPa (with scatter <±13 GPa) respectively. The corresponding hardness and modulus of untreated Ti-6Al-4V were ~4.1 (±0.62) and ~148 (±7) GPa respectively. Laser processing at power densities >35 W/mm(2) enhanced the surface properties (as passive current density is reduced) so that the materials may be suitable for the biomedical applications.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Electrochemical Corrosion Behavior of Ta2N Nanoceramic Coating in Simulated Body Fluid

In order to improve the corrosion and wear resistance of biomedical Ti-6Al-4V implants, a Ta₂N nanoceramic coating was synthesized on a Ti-6Al-4V substrate by the double glow discharge plasma process. The Ta₂N coating, composed of fine nanocrystals, with an average grain size of 12.8 nm, improved the surface hardness of Ti-6Al-4V and showed good contact damage tolerance and good adhesion streng...

متن کامل

Effect of Procedure Time on Microstructure and Corrosion Behavior of ZrTiO4/ZrO2 Nanocomposite Coatings by Plasma Electrolytic Oxidation (PEO) Applied on the Ti-6Al-4V Substrate

In this research, the effect of PEO procedure time on the distinct properties of coatings such as morphology, chemical composition, roughness and corrosion has been studied. A scanning electron microscopy equipped with an energy dispersive spectroscopy was used to study the microstructure of the coatings. In addition, x-ray diffraction (XRD) and roughness meter were used to evaluate the chemica...

متن کامل

Investigation of the effect of temperature on the corrosion behavior of welded joints similar of titanium alloy Ti-6Al-4V by friction stir welding method

In this study, corrosion behavior of Ti-6Al-4V titanium alloy joint by friction stir welding with a rotational speed of 375 rpm and a travel speed of 100 mm/min was investigated. The welding procedure was carried out under β-transus temperature that was consisted of equiaxed grains in the stir zone. The corrosion behavior of the welded joint was investigated in 3.5% NaCl solution at temperature...

متن کامل

Mechanical Surface Treatments of Ti-6Al-4V Miniplate Implant Manufactured by Electrical Discharge Machining (TECHNICAL NOTE)

Present work aims at multi-mechanical surface treatment of Ti-6Al-4V based-miniplate implant manufactured by electrical discharge machining (EDM) for biomedical use. Mechanical surface treatment consists of consequent use of ultrasonic cleaning, rotary tumbler polishing, and brushing. Surface layers are analyzed employing scanning electron microscopy and energy dispersive X-ray spectroscopy. Al...

متن کامل

Investigation of the effect of temperature on the corrosion behavior of welded joints similar of titanium alloy Ti-6Al-4V by friction stir welding method

In this study, corrosion behavior of Ti-6Al-4V titanium alloy joint by friction stir welding with a rotational speed of 375 rpm and a travel speed of 100 mm/min was investigated. The welding procedure was carried out under β-transus temperature that was consisted of equiaxed grains in the stir zone. The corrosion behavior of the welded joint was investigated in 3.5% NaCl solution at temperature...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of materials science. Materials in medicine

دوره 22 8  شماره 

صفحات  -

تاریخ انتشار 2011