Radiographic inspection of porosity in Ti-6Al-4V laser-welded joints.
نویسندگان
چکیده
Widely used in dentistry, Ti-6Al-4V alloy is difficult to cast and solder, as it frequently exhibits pores inside the structure. This study was conducted to evaluate the effect of joint openings and diameters of laser-welded joints executed in Ti-6Al-4V structures on the presence of pores as checked by radiographic procedures. Sixty dumbbell rods with central diameters of 1.5, 2.0 and 3.5 mm were created from Ti-6Al-4V-wrought bars. Specimens were sectioned and welded using two joint openings (0.0 and 0.6 mm). The combination of variables created six groups (n = 10). Laser welding was executed using 360V/8ms (1.5 and 2.0 mm) and 380V/9ms (3.5 mm), with the focus and frequency set to zero. The joints were finished, polished and submitted to radiographic examination. The radiographs were visually examined for the presence of pores in the joints, qualitatively. The percentage of radiographic presence of pores was calculated without counting pores per joint. Data were analyzed using a chi-square test (α = 0.05). For the 1.5-mm specimens, the incidence of pore presence was significantly higher (p = 0.0001) when using 0.6-mm joint openings (40%) compared to 0.0-mm openings (0%). For the 2.0-mm specimens, there was no significant difference between groups (p = 0.2008). However, for the 3.5-mm specimens, the incidence of pore presence was lower (p = 0.0061) for 0.6-mm openings (50%) compared to 0.0-mm openings (70%). Therefore, laser welding of Ti-6Al-4V structures with thin diameters provides the best condition for the juxtaposition of the parts.
منابع مشابه
Investigation of the effect of temperature on the corrosion behavior of welded joints similar of titanium alloy Ti-6Al-4V by friction stir welding method
In this study, corrosion behavior of Ti-6Al-4V titanium alloy joint by friction stir welding with a rotational speed of 375 rpm and a travel speed of 100 mm/min was investigated. The welding procedure was carried out under β-transus temperature that was consisted of equiaxed grains in the stir zone. The corrosion behavior of the welded joint was investigated in 3.5% NaCl solution at temperature...
متن کاملEffect of Laser Spot Welding Variables on Microstructure and Mechanical Properties of the Ti-6AL-4V to AISI304 Dissimilar Joint
In this project, joining Ti-6Al-4V and AISI 304 dissimilar plates by laser-spot-welding method has been studied. In this regard, Ti-6Al-4V and AISI 304 plates, with a thickness of 0.7 and 0.5 respectively, were lap-welded using an interlayer of 0.2 & 0.3 mm copper and silver (pure silver). The process was done by 400Watt pulsed laser (Nd:YAG) using oncentric spot welding with 4mm diameter circl...
متن کاملEffect of Laser Spot Welding Variables on Microstructure and Mechanical Properties of the Ti-6AL-4V to AISI304 Dissimilar Joint
In this project, joining Ti-6Al-4V and AISI 304 dissimilar plates by laser-spot-welding method has been studied. In this regard, Ti-6Al-4V and AISI 304 plates, with a thickness of 0.7 and 0.5 respectively, were lap-welded using an interlayer of 0.2 & 0.3 mm copper and silver (pure silver). The process was done by 400Watt pulsed laser (Nd:YAG) using oncentric spot welding with 4mm diameter circl...
متن کاملInvestigation of the effect of temperature on the corrosion behavior of welded joints similar of titanium alloy Ti-6Al-4V by friction stir welding method
In this study, corrosion behavior of Ti-6Al-4V titanium alloy joint by friction stir welding with a rotational speed of 375 rpm and a travel speed of 100 mm/min was investigated. The welding procedure was carried out under β-transus temperature that was consisted of equiaxed grains in the stir zone. The corrosion behavior of the welded joint was investigated in 3.5% NaCl solution at temperature...
متن کاملTi-6Al-4V triply periodic minimal surface structures for bone implants fabricated via selective laser melting.
Triply periodic minimal surface (TPMS) structures have already been shown to be a versatile source of biomorphic scaffold designs. Therefore, in this work, Ti-6Al-4V Gyroid and Diamond TPMS lattices having an interconnected high porosity of 80-95% and pore sizes in the range of 560-1600 μm and 480-1450 μm respectively were manufactured by selective laser melting (SLM) for bone implants. The man...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Brazilian oral research
دوره 25 2 شماره
صفحات -
تاریخ انتشار 2011