Effect of Metal Primers on Bond Strength of a Composite Resin to Nickel-Chrome Metal Alloy.

نویسندگان

  • Gabriel Nima
  • Paulo Vitor Campos Ferreira
  • Andreia Bolzan de Paula
  • Simonides Consani
  • Marcelo Giannini
چکیده

This study evaluated the effects of three metal primers and one multi-mode adhesive system on the shear bond strength (SBS) of a flowable composite resin to nickel-chrome metal alloy (Ni-Cr). Ninety plates were cast from Ni-Cr and divided in nine groups (n=10). The surfaces were sandblasted with Al2O3 and primed with three adhesive primers: Alloy Primer (AP), Universal Primer (TP) and RelyX Ceramic Primer (CP), and a multi-mode adhesive (Scotchbond Universal, SU). The Adper Single Bond Plus (SB) and SU adhesives were also combined with adhesive primers. Control group did not have any surface treatment. The groups were: AP, AP+SB, AP+SU, TP+SB, TP+SU, CP+SB, CP+SU and SU. Composite cylinders were built on alloy surface. After 24 h, half the specimens were subjected to SBS and the other half to thermal cycling before testing. Data were analyzed by two-way ANOVA and Tukey's test (a=0.05). Failure modes were assessed by SEM observation. Higher SBS were obtained with AP and TP combined with adhesives at 24 h and the lowest one for control group. Thermocycling reduced SBS for AP, CP+SU and SU. Combination between TP and SU resulted in the highest SBS after the thermocycling. TP groups showed all types of failures and high incidence of mixed failures. The use of AP and UP metal primers before application of SU and SB adhesive systems increased the SBS of composite to Ni-Cr. These combinations between metal primers and adhesives had the highest SBS after thermocycling.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Type of Surface Treatment and Adhesive System on Shear Bond Strength of Composite Resin to a Non-Precious Metal Alloy

Background and Aim: Fractured metal-ceramic restorations may be repaired with composite in some cases to postpone the fabrication of a new restoration. Knowledge about the bond strength can help predict the success rate of this treatment modality. The aim of this study was to assess the effect of two types of mechanical surface treatment of metal along with the use of different adhesive systems...

متن کامل

Effect of metal primers and tarnish treatment on bonding between dental alloys and veneer resin

PURPOSE The aim of this study was to evaluate the effect of metal primers on the bonding of dental alloys and veneer resin. Polyvinylpyrrolidone solution's tarnish effect on bonding strength was also investigated. MATERIALS AND METHODS Disk-shape metal specimens (diameter 8 mm, thickness 1.5 mm) were made from 3 kinds of alloy (Co-Cr, Ti and Au-Ag-Pd alloy) and divided into 4 groups per each ...

متن کامل

Effect of Sulfur-Containing Primers for Noble Metals on the Bond Strength of Self-Cured Acrylic Resin

This study investigated the effect of sulfur-containing primers for noble metals on the shear bond strength of self-cured acrylic resin after thermal cycling (TC). Four pure metals (Au, Ag, Cu, and Pd) and type IV Au alloy were either untreated, or treated with one of the five sulfur-containing metal primers (V-Primer, Metaltite, Alloy Primer, Metal Link Primer, and Metal Primer Z). Afterwards,...

متن کامل

Comparison of the effect of different surface treatments on the bond strength of different cements with nickel chromium metal alloy: An in vitro study

BACKGROUND For success of any indirect metal restoration, a strong bond between cement and the intaglio surface of metal is imperative. The aim of this study is to evaluate and compare the effect of different surface treatment on the tensile and shear bond strength of different cements with nickel-chromium alloy. MATERIAL AND METHODS 120 premolars were sectioned horizontally parallel to the o...

متن کامل

Effect of Primers on the Shear Bond Strength of Two Types of Acrylic Resin to Co-cr Partial Denture Alloy

The absence or poor chemical bonding of acrylic resin to Cobalt-Chromium metal frameworks, often introduces microleakage and bond failure at the interface. The aim of this study was to compare the shear bond strength of sandblasted cast and ingot cobaltchromium alloy to heat-cured and self-cured acrylic resins primed with four different metal primers. Fifty Co-Cr Ingot and fifty cast specimens ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Brazilian dental journal

دوره 28 2  شماره 

صفحات  -