Wear Behavior of Fiber Laser Textured TiN Coatings in a Heavy Loaded Sliding Regime
نویسندگان
چکیده
In heavy loaded mating components, such as sliders and sliding bearings, guaranteeing the efficiency of lubricant films for long times during severe service conditions is very complicated. In this work, the benefits deriving from the use of fiber laser sources for surface texturing of very thin TiN coatings in severe wear working conditions were demonstrated. Evaluations of the laser textured dimples shape, geometry and density are given. Wear performance of the fiber laser textured surfaces was evaluated in discontinuous oil lubricated conditions with a flat contact. High normal load and low sliding speed were applied. Comparison tests were also performed on commercial TiN and WC/C coatings. In terms of average wear volume and maximum wear depth, Laser Surface Texturing of TiN provided respectively a 70% and a 45% reduction if compared to plain TiN. If compared to WC/C the wear resistance gains were lower but LST TiN maintained such benefits for longer wear runs. SEM analysis also revealed that the laser interaction provided a localized thermal cracking to the TiN coating. However, the sliding action caused very limited and localized coating fragmentation or delamination.
منابع مشابه
COMPARISON OF THE CrN , TiN AND (Ti, Cr)N PVD COATINGS DEPOSITED BY CATHODIC ARC EVAPORATION
In the present study, CrN, TiN and (Ti, Cr)N coatings were deposited on D6 tool steel substrates. Physical and mechanical properties of coatings such as microstructure, thickness, phase composition, and hardness were evaluated. Phase compositions were studies by X-ray diffraction method. Mechanical properties were determined by nano-indentation technique. The friction and wear behaviour of the ...
متن کاملEffect of NiTi Addition on the Wear Resistance of YSZ Coatings
In this study, small fraction of NiTi (5 wt%) was added to Yttria stabilized zirconia (YSZ) top coat to improve it sliding wear resistance. The measurement of width of wear tracks after wear tests under a 15 N load for 100 m sliding distances showed that the width of wear track in NiTi-YSZ coating is shorter than that in YSZ coating which depicts the higher wear resistance of NiTi-YSZ coa...
متن کاملCharacterization of CrN/TiN PVD Coatings on 316L Stainless Steel
In order to further enhance tribological properties 316 Low carbon stainless steel (L SS) used on mechanical parts. CrN/TiN with DC magnetron sputtering sources was carried out on PVD 316 L SS. The micro structure of the CrN/TiN coatings were investigated by Scanning electron microscope (SEM), X-ray Diffraction (XRD) and tribology properties were investigated on a Pin on Disc friction and wear ...
متن کاملDry Friction and Wear Performance of Micro Surface Textures Generated by Ultrasonic Assisted Face Turning
Nowadays the surface texturing has been widely recognized as a usable capability to improve the tribological systems. In this paper, ultrasonic assisted turning (UAT) isperformed to create the micro textures on the flat faces. Micro surface texturing ismade on the Al7075-T6 by the UAT in the face turning process. Then, the influences of cutting speed feed, vibration direction and vibration ampl...
متن کاملDry Friction and Wear Performance of Micro Surface Textures Generated by Ultrasonic Assisted Face Turning
Nowadays the surface texturing has been widely recognized as a usable capability to improve the tribological systems. In this paper, ultrasonic assisted turning (UAT) isperformed to create the micro textures on the flat faces. Micro surface texturing ismade on the Al7075-T6 by the UAT in the face turning process. Then, the influences of cutting speed feed, vibration direction and vibration ampl...
متن کامل