Retrieval analysis of squeaking alumina ceramic-on-ceramic bearings.

نویسندگان

  • W L Walter
  • S M Kurtz
  • C Esposito
  • W Hozack
  • K G Holley
  • J P Garino
  • M A Tuke
چکیده

This multicentre study analysed 12 alumina ceramic-on-ceramic components retrieved from squeaking total hip replacements after a mean of 23 months in situ (11 to 61). The rates and patterns of wear seen in these squeaking hips were compared with those seen in matched controls using retrieval data from 33 'silent' hip replacements with similar ceramic bearings. All 12 bearings showed evidence characteristic of edge-loading wear. The median rate of volumetric wear was 3.4 mm(3)/year for the acetabular component, 2.9 mm(3)/year on the femoral heads and 6.3 mm(3)/year for head and insert combined. This was up to 45 times greater than that of previously reported silent ceramic-on-ceramic retrievals. The rate of wear seen in ceramic components revised for squeaking hips appears to be much greater than in that seen in retrievals from 'silent' hips.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

High survivorship with a titanium-encased alumina ceramic bearing for total hip arthroplasty.

BACKGROUND Although ceramic-on-ceramic bearings for total hip arthroplasty (THA) show promising results in terms of bearing-surface wear, fracture of the bearing, insertional chips, and squeaking remain a concern. QUESTIONS/PURPOSES Our primary objective of this report was to determine overall survivorship of a titanium-encased ceramic-on-ceramic bearing couple. Our secondary objectives were ...

متن کامل

In Vitro and in Vivo Analysis of Squeaking Frequencies in Ceramic-on-ceramic Total Hip Prosthesis

INTRODUCTION: Squeaking after total hip replacement has been reported in up to 10% of patients (1). Some authors proposed that sound emissions from squeaking hips result from resonance of one or other or both of the metal parts and not the bearing surfaces (2). There is no reported in vitro study about the squeaking frequencies under lubricated regime. The goal of the study was to reproduce the...

متن کامل

Retrieval analysis of alumina ceramic-on-ceramic bearing couples

BACKGROUND AND PURPOSE Ceramic-on-ceramic (CoC) bearings have been in use in total hip replacement (THR) for more than 40 years, with excellent long-term survivorship. Although there have been several simulator studies describing the performance of these joints, there have only been a few retrieval analyses. The aim of this study was to investigate the wear patterns, the surface properties, and...

متن کامل

Microseparation and stripe wear in alumina-on-alumina hip implants.

The combination of materials that still has highest wear resistance for total hip replacement is ceramic-on-ceramic. However, brittleness is a major concern for ceramics: in vivo and in vitro studies on ceramic hip prostheses correlate microseparation with hip noise, ceramic wear, or ceramic liner damage. Ceramic microseparation can lead to edge load, ceramic head wear, and squeaking. The aim o...

متن کامل

Fracture of ceramic components as a serious failure after total hip replacement with ceramic-on-ceramic bearings

Introduction Ceramics have been introduced in total hip arthroplasty for several advantages including minimal friction, low wear, biocompatibility, no ageing problems and no problems related to the systemic increases in serum metal concentrations. In the first generation of ceramic components introduced in the 1970’s the risk of fracture was substantial, reaching up to 13.4 %. After introducing...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • The Journal of bone and joint surgery. British volume

دوره 93 12  شماره 

صفحات  -

تاریخ انتشار 2011