OBJECTIVE The aim of this study was to assess whether repetitive opening and closure of self-ligating bracket clips can cause plastic deformation of the clip. METHODS Three types of active/interactive ceramic self-ligating brackets (n = 20) were tested: In-Ovation C, Quicklear and WOW. A standardized controlled device performed 500 cycles of opening and closure movements of the bracket clip with proper instruments and techniques adapted as recommended by the manufacturer of each bracket type. Two tensile tests, one before and one after the repetitive cycles, were performed to assess the stiffness of the clips. To this end, a custom-made stainless steel 0.40 x 0.40 mm wire was inserted into the bracket slot and adapted to the universal testing machine (EMIC DL2000), after which measurements were recorded. On the loading portion of the loading-unloading curve of clips, the slope fitted a first-degree equation curve to determine the stiffness/deflection rate of the clip. RESULTS The results of plastic deformation showed no significant difference among bracket types before and after the 500 cycles of opening and closure (p = 0.811). There were significant differences on stiffness among the three types of brackets (p = 0.005). The WOW bracket had higher mean values, whereas Quicklear bracket had lower values, regardless of the opening/closure cycle. CONCLUSION Repetitive controlled opening and closure movements of the clip did not alter stiffness or cause plastic deformation.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Torque expression of self-ligating brackets compared with conventional metallic, ceramic, and plastic brackets.

The purpose of this research was to investigate the torque capacity of active and passive self-ligating brackets compared with metallic, ceramic, and polycarbonate edgewise brackets. Six types of orthodontic brackets were included in the study: the self-ligating Speed and Damon2, the stainless steel (SS), Ultratrimm and Discovery, the ceramic bracket, Fascination 2, and the polycarbonate bracke...

متن کامل

A comparative study of frictional force in self-ligating brackets according to the bracket-archwire angulation, bracket material, and wire type

OBJECTIVE This study aimed to compare the frictional force (FR) in self-ligating brackets among different bracket-archwire angles, bracket materials, and archwire types. METHODS Passive and active metal self-ligating brackets and active ceramic self-ligating brackets were included as experimental groups, while conventional twin metal brackets served as a control group. All brackets were maxil...

متن کامل

Opening and closure forces of sliding mechanisms of different self-ligating brackets

UNLABELLED Self-ligating brackets engage the wire by means of a slide mechanism. Forces that have to be applied to open and close the sliding mechanism of brackets are still unknown. OBJECTIVE The aim of this study was to measure and compare the opening and closure forces of different self-ligating brackets. MATERIAL AND METHODS Three different stainless steel self-ligating brackets (Carrie...

متن کامل

Frictional Resistance of Three Types of Ceramic Brackets

OBJECTIVES To investigate the static frictional resistance at the bracket/archwire interface in two recently introduced bracket systems and compare them to conventional ceramic and conventional metal bracket systems. Three variables were considered including the bracket system, archwire type and archwire angulation. MATERIAL AND METHODS Four bracket systems were tested in vitro: Self ligating...

متن کامل

Assessment of Bracket Surface Morphology and Dimensional Change

OBJECTIVE The objective of this study was to compare the surface morphology and dimensional stability of the bracket slot at the onset of treatment and after 12 months of intraoral exposure. The study also compared the amount of calcium at the bracket base which indicates enamel loss among the three orthodontic brackets following debonding after 12 months of intraoral exposure. MATERIALS AND ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Dental press journal of orthodontics

دوره 20 4  شماره 

صفحات  -

تاریخ انتشار 2015