Novel silane encapsulation system for tribochemical resin bonding to a Co-Cr alloy.
نویسندگان
چکیده
OBJECTIVES Encapsulated silane has been introduced in powders for tribochemical coating (SilJet Plus, SP), eliminating the need for a separate silane primer. The aim of the study was to comparatively evaluate the effect of SP on the surface properties and bond strength of a Co-Cr alloy with a resin composite. METHODS Co-Cr cast alloy disks were subjected to tribochemical treatments with CoJet (CJ), SilJet (SJ) and SP. Polished specimens were used as control (CR). The alloy surfaces were studied by optical profilometry (OIP; parameters Sa,Sz,Sdr,Sci), reflection FTIR microscopy (RFTIRM; CR,CJ,SJ silanized with S-Bond), scanning electron microscopy/energy dispersive X-ray microanalysis (SEM/EDX; Al+Si coverage), contact angle with water (CW) and shear bond strength with a flowable resin composite (SBS). Statistical analysis for OIP, Al+Si coverage, CW and SBS was performed by one-way ANOVA and Holm-Sidak multiple comparison tests and by Chi-square for the failure mode (α=0.05). RESULTS CR demonstrated the lowest Sa,Sz,Sdr values from all sandblasted surfaces, excluding Sci of SJ. Among tribochemical treatments, no differences were found in Sa,Sz. CJ showed lower Sdr and SJ higher Sci. The peaks of SiO were very weak on CR, but detectable on CJ, SJ and SP, with no evidence of SiOCH3 groups. The ranking of the statistical significant differences in CW measurements was SP>SJ+silane>CJ+silane>CR+silane. Well-defined Al and diffuse Si distributions were found on the alloy surface following tribochemical treatments. The maximum Al+Si coverage ranged between 50 and 54% (5000×) and the random coverage between 7 and 11% (1000×, p>0.05 for both). Tribochemical treatments showed higher SBS from CR (p<0.05), but with no statistically significant differences among them. CR demonstrated exclusively adhesive failures, whereas in tribochemically coated groups adhesive failures ranged from 10 to 20%. CLINICAL SIGNIFICANCE Tribochemical treatments with encapsulated silane may be considered an efficient single-step alternative to conventional two-step systems for bonding to Co-Cr alloys, offering a significant reduction in chairside time.
منابع مشابه
Factors affecting the bond strength of denture base and reline acrylic resins to base metal materials
OBJECTIVE The shear bond strengths of two hard chairside reline resin materials and an auto-polymerizing denture base resin material to cast Ti and a Co-Cr alloy treated using four conditioning methods were investigated. MATERIAL AND METHODS Disk specimens (diameter 10 mm and thickness 2.5 mm) were cast from pure Ti and Co-Cr alloy. The specimens were wet-ground to a final surface finish of 6...
متن کاملEffect of metal primers and tarnish treatment on bonding between dental alloys and veneer resin
PURPOSE The aim of this study was to evaluate the effect of metal primers on the bonding of dental alloys and veneer resin. Polyvinylpyrrolidone solution's tarnish effect on bonding strength was also investigated. MATERIALS AND METHODS Disk-shape metal specimens (diameter 8 mm, thickness 1.5 mm) were made from 3 kinds of alloy (Co-Cr, Ti and Au-Ag-Pd alloy) and divided into 4 groups per each ...
متن کاملBonding strength of resin cement to silicate glass ceramics for dental CAD/CAM systems is enhanced by combination treatment of the bonding surface.
To increase the bond strength of CAD/CAM-fabricated, leucite-reinforced glass ceramics with a resin cement, the effects of the following were investigated: surface modification by tribochemical (TBC) treatment, followed by combined application of a silane coupling agent and a functional monomer as a primer. Bond strength was evaluated by a shear bond test. It was found that a silane coupling ag...
متن کاملSpark erosion as a metal-resin bonding system.
PURPOSE Resin to metal bond strength of two commercial and one experimental metal-resin bonding system for crown and bridge veneer composites was evaluated. MATERIALS AND METHODS All specimens were prepared and tested according to ISO 10477 Amendment 1. A high precious alloy (HPA), a Co/Cr-alloy (Co/Cr) and pure titanium (Ti) were wet-ground to a final surface finish of 800 grit and air-dried...
متن کاملScientific Efficacy of a Combined Silica/methacrylate Coupling on the Fiber Post Bonding to Composite Cores
58 INTERNATIONAL DENTISTRY SA VOL. 8, NO. 4 Introduction The clinical success of fiber post-retained restorations depends on the establishment of a reliable bond at the root-post-core interfaces. In spite of the improvements in dental material technology, post to composite adhesion is still considered relatively low. Advances in silane coupling agents enhance bond strength by promoting adhesion...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Journal of dentistry
دوره 50 شماره
صفحات -
تاریخ انتشار 2016