This paper presents the application of a life fraction hardening rule to the analytical calculation of creep in hot section components. Accurate prediction of creep is critical to assuring the mechanical integrity of heavy-duty, industrial gas turbine (IGT) hardware. The accuracy of such predictions depend upon both the creep models assumed and how those models are implemented in a finite element solution. A modified theta projection creep model for a nickel-based super alloy was presented in a previous paper as an accurate simulation of creep behavior [1]. Application of such a user defined creep law depends upon definition of a hardening rule in the form of either an explicit or an implicit integration scheme in order to calculate incremental strains during any time increment. Time hardening is the simplest and least computationally intensive of the two most common hardening rules, but does not correctly show the effect of changing stresses or temperatures. Strain hardening may provide the most accurate solution, but the creep models are too complex to invert, which results in highly iterative and computationally intensive solutions. A life fraction hardening rule has been presented in other works [2] as a compromise between time hardening and strain hardening. Life fraction hardening is presented here as a highly efficient and accurate means of calculating incremental creep strain when applied to a modified theta projection creep model. A user creep subroutine was defined using a state variable to represent the strain life fraction at any time. By using the time to tertiary creep as the denominator for the life fraction, no new material constants are needed to relate to creep failure. The start of tertiary creep is effectively considered to be a failure. Additional design insight can be provided through the inclusion of other state variables to calculate temperature margins at current conditions. Material testing with changing stress levels will be used to help validate the technique. A simplified example of the technique is presented in the paper. More accurate creep predictions allow our company to improve the structural integrity of its turbine blades and vanes.
منابع مشابه
Effect of Overage Hardening Heat Treatment on the Micro Structure and Hardness of Nickel-based Super Alloy Rene-80
Rene-80 nickel-base superalloy as an alloy for production of the jet turbine blades shows high mechanical properties as well as microstructure stability during the high temperature engine operation. In this research, age hardening heat treatment cycle was done on the as-cast Rene-80 superalloy. In the following, microstructure, elemental analysis of phases and macro-hardness of the alloy before...
متن کاملA Model for Creep and Creep Damage in the γ-Titanium Aluminide Ti-45Al-2Mn-2Nb
Gamma titanium aluminides (γ-TiAl) display significantly improved high temperature mechanical properties over conventional titanium alloys. Due to their low densities, these alloys are increasingly becoming strong candidates to replace nickel-base superalloys in future gas turbine aeroengine components. To determine the safe operating life of such components, a good understanding of their creep...
متن کاملHold-time Effects on Low-cycle-fatigue Behavior of Hastelloy® X Superalloy at High Temperatures
Total strain-controlled low-cycle-fatigue tests with and without hold times were performed at temperatures ranging from 816°C to 982°C in a laboratory air on a nickel-based superalloy, HASTELLOY X. The influence of hold times on the cyclicstress response and fatigue life was studied. At the temperatures considered, the alloy exhibited initial cyclic hardening, followed by a saturated cyclic-str...
متن کاملCreep Life Forecasting of Weldment
One of the yet unresolved engineering problems is forecasting the creep lives of weldment in a pragmatic way with sufficient accuracy. There are number of obstacles to circumvent including: complex material behavior, lack of accurate knowledge about the creep material behavior specially about the heat affected zones (HAZ),accurate and multi-axial creep damage models, etc. In general, creep life...
متن کاملCreep Life Assessment of Primary Reformer HP40-NB Modified Steel Tube of an Ammonia Plant
Assessment of creep damage and residual creep life of a cast HP 40 Nb Mod. Reformer tube was performed, wherein the experimental Larson–Miller diagram and area fraction of creep voids were adopted. The state of damage of the tube in service was metallographically analyzed by using light and electron microscopy. Samples from the serviced reformer furnace tube were cut and prepared for void exami...
متن کامل