Deflection test evaluation of different lots of the same nickel-titanium wire commercial brand.
نویسندگان
چکیده
INTRODUCTION The aim of this in vitro study was to compare the elastic properties of the load-deflection ratio of orthodontic wires of different lot numbers and the same commercial brand. METHODS A total of 40 nickel-titanium (NiTi) wire segments (Morelli Ortodontia™--Sorocaba, SP, Brazil), 0.016-in in diameter were used. Groups were sorted according to lot numbers (lots 1, 2, 3 and 4). 28-mm length segments from the straight portion (ends) of archwires were used. Deflection tests were performed in an EMIC universal testing machine with 5-N load cell at 1 mm/minute speed. Force at deactivation was recorded at 0.5, 1, 2 and 3 mm deflection. Analysis of variance (ANOVA) was used to compare differences between group means. RESULTS When comparing the force of groups at the same deflection (3, 2 and 1 mm), during deactivation, no statistical differences were found. CONCLUSION There are no changes in the elastic properties of different lots of the same commercial brand; thus, the use of different lots of the orthodontic wires used in this research does not compromise the final outcomes of the load-deflection ratio.
منابع مشابه
The influence of distal-end heat treatment on deflection of nickel-titanium archwire
OBJECTIVE The aim of this in vitro study was to evaluate the deflection-force behavior of nickel-titanium (NiTi) orthodontic wires adjacent to the portion submitted to heat treatment. MATERIAL AND METHODS A total of 106 segments of NiTi wires (0.019 x 0.025-in) and heat-activated NiTi wires (0.016 x 0.022-in) from four commercial brands were tested. The segments were obtained from 80 archwire...
متن کاملLoad Deflection Characteristics of Nickel Titanium Initial Archwires.
OBJECTIVES The aim of this study was to assess and compare the characteristics of commonly used initial archwires by their load deflection graphs. MATERIALS AND METHODS This study tested three wire designs namely copper nickel titanium (CNT), nickel titanium (NiTi), and multi-strand NiTi (MSNT) archwires engaged in passive self-ligating (PSL) brackets, active self-ligating (ASL) brackets or c...
متن کاملAngular deflection of rotary nickel titanium files: a comparative study.
A new manufacturing method of twisting nickel titanium wire to produce rotary nickel titanium (RNT) files has recently been developed. The aim of the present study was to evaluate whether the new manufacturing process increased the angular deflection of RNT files, by comparing instruments produced using the new manufacturing method (Twisted Files) versus instruments produced with the traditiona...
متن کاملEvaluation of deflection forces of orthodontic wires with different ligation types.
The aim of this study was to evaluate deflection forces of orthodontic wires of different alloys engaged into conventional brackets using several ligation types. Stainless steel, conventional superelastic nickel-titanium and thermally activated nickel-titanium archwires tied into conventional brackets by a ring-shaped elastomeric ligature (RSEL), a 8-shaped elastomeric ligature (8SEL) and a met...
متن کاملComparison of the superelasticity of different nickel–titanium orthodontic archwires and the loss of their properties by heat treatment
The aim of this work is to describe and compare mechanical properties of eight widely used nickel-titanium orthodontic wires under uniform testing conditions and to determine the influence of the heat treatments on the loss of the superelasticity. Ten archwires from two batches from eight different manufacturers were evaluated. A three-point bending test was performed, in accordance with ISO 15...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Dental press journal of orthodontics
دوره 21 1 شماره
صفحات -
تاریخ انتشار 2016