Corrosion Behavior of Ti60 Alloy under a Solid NaCl Deposit in Wet Oxygen Flow at 600 °C

نویسندگان

  • Lei Fan
  • Li Liu
  • Zhongfen Yu
  • Min Cao
  • Ying Li
  • Fuhui Wang
چکیده

The corrosion behavior of Ti60 alloy covered with a solid NaCl deposit in wet oxygen flow at 600 °C has been studied further by SEM, EDX, XPS, XRD, TEM and EPMA analysis. The results show that solid NaCl and H2O react with Ti oxides, which destroyed the Ti oxide scale to yield the non-protective Na4Ti5O12 and other volatile species. The resulting corrosion product scale was multilayered and contained abundant rapid diffusion channels leading to the fast diffusion which improved the corrosion rate. A possible mechanism has been proposed for the NaCl-covered Ti60 alloy, based on the experimental results.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Corrosion Behavior of Pure Ti under a Solid NaCl Deposit in a Wet Oxygen Flow at 600 C

The corrosion behavior of pure Ti under a solid NaCl deposit in a wet O2 flow at 600 ̋C has been studied. The results showed that the corrosion rate was greatly accelerated by solid NaCl, which destroyed the compact and protective TiO2 scale to yield non-protective N4Ti5O12 and other products. Detailed scanning electron microscopy (SEM) equipped with an energy dispersive spectrometer (EDX), and...

متن کامل

The Corrosion Behavior of Pure Iron under Solid Na2SO4 Deposit in Wet Oxygen Flow at 500 °C

The corrosion behavior of pure Fe under a Na₂SO₄ deposit in an atmosphere of O₂ + H₂O was investigated at 500 °C by thermo gravimetric, and electrochemical measurements, viz. potentiodynamic polarization, electrochemical impedance spectroscopy (EIS), and surface characterization methods viz. X-ray diffraction (XRD), and scanning electron microscope (SEM)/energy dispersive spectroscopy(EDS). The...

متن کامل

Investigation of the effect of temperature on the corrosion behavior of welded joints similar of titanium alloy Ti-6Al-4V by friction stir welding method

In this study, corrosion behavior of Ti-6Al-4V titanium alloy joint by friction stir welding with a rotational speed of 375 rpm and a travel speed of 100 mm/min was investigated. The welding procedure was carried out under β-transus temperature that was consisted of equiaxed grains in the stir zone. The corrosion behavior of the welded joint was investigated in 3.5% NaCl solution at temperature...

متن کامل

Investigation of the effect of temperature on the corrosion behavior of welded joints similar of titanium alloy Ti-6Al-4V by friction stir welding method

In this study, corrosion behavior of Ti-6Al-4V titanium alloy joint by friction stir welding with a rotational speed of 375 rpm and a travel speed of 100 mm/min was investigated. The welding procedure was carried out under β-transus temperature that was consisted of equiaxed grains in the stir zone. The corrosion behavior of the welded joint was investigated in 3.5% NaCl solution at temperature...

متن کامل

Effect of ageing heat treatment on corrosion behaviorof 17-4 PH stainless steel in 3.5% NaCl

The 17-4PH alloy is a martensitic stainless steel with 3–5 wt% Cu, strengthened by the precipitation hardening. Due to excellent mechanical properties, corrosion resistance and ease of heat treatment, this alloy has unique applications in nuclear power plants and marine constructions. In this paper, the influence of ageing heat treatment, solution annealing followed by ageing at 480, 550 and 62...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 6  شماره 

صفحات  -

تاریخ انتشار 2016