Xu, Lei and Zhang, Shu-Yan and Sun, Wei and McCartney, David G. and Hyde, Thomas H. and James, Jon and Drakopoulos, Michael (2015) Residual stress distribution in a Ti-6Al-4V T-joint weld measured using synchrotron X-ray diffraction. The Journal of Strain

ثبت نشده
چکیده

To improve the manufacturing quality of welded structures, to prevent failures at weld joints and to predict their lifetime, measurements of the residual stresses generated by welding in the structures are extremely useful. The residual stresses may reduce the component life due to phenomena that occur at low applied stresses such as brittle fracture, fatigue and stress corrosion cracking. Welded thin Ti-6Al-4V panel components are commonly found in aeroengine assemblies and the weld integrity and reliability are critical. In this work, the residual stress distributions in a welded thin Ti-6Al-4V T-joint were measured by the newly developed SScanSS program with synchrotron X-ray diffraction technique. The measurement performed in this study, which included a large number of measurement points, has mapped a complete stress field in a thin sheet T-joint weld. It has not only provided improved understanding of residual stress in such a joint but also filled the missing link between the residual stress obtained by numerical modelling and their validation. The results have shown that the longitudinal stresses play the most important role in the residual stress distribution over the flange and high tensile stresses appear in the region near the weld zone. The measured results were compared with numerically predicted results and these showed good agreement.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

TIG Surface Alloying of Ti-6Al-4V with Nitrogen and Chromium for Improved Tribological Properties

Due to special properties such as low density, high strength and high corrosion resistance Ti-6Al-4V alloy has been used extensively in various industries, especially in the aerospace aspects. However the major problem of this alloy is its poor tribological properties under relatively high loads. In the present study, in order to improve the tribological properties of mentioned alloy, chromium ...

متن کامل

Evaluating the Effect of the Number of Welding Passes on Microstructure, Hardness and Residual Stress of Ti-Al-Si Composite Coatings

The purpose of the present work is to investigate the influence of the number of weld-passes on microstructure, hardness and residual stresses of composite coatings composed of Ti-Al-Si intermetallic compounds. In this regard, surface coating of pure Ti was carried out using one and two passes of tungsten inert gas (TIG) welding with an Al filler alloy (grade 4043). Phase and structural evaluat...

متن کامل

Investigation of the mechanical properties and microstructure of the Ti-6Al-4V to Al2024 joint fabricated by successive- stage transient liquid phase (S-TLP) method

The aim of this study is investigation of TLP variables on microstructure and mechanical properties of Al2024 to Ti-6Al-4V bonding for TLP joint. For this purpose, the sheets were prepared with dimension of 130×32×3 mm from Ti-6Al-4V and Al2024 alloys and 50µm thick Sn-5.3Ag-4.2Bi foil as interlayer. Sn-5.3Ag-4.2Bi foil prepared with dimension of 32×25 mm. Two alloys was joint together by proce...

متن کامل

DIRECT LASER DEPOSITION OF Ti-6Al-4V FROM ELEMENTAL POWDER BLENDS

A thin-wall structure composed of Ti-6Al-4V has been deposited using direct laser deposition (DLD) from blended Ti, Al, and V elemental powders. The microstructure and composition distribution along the build height direction were intensively investigated using optical microscopy, scanning electron microscopy/energy dispersive X-ray spectroscopy (SEM/EDS), and Vickers hardness testing. The micr...

متن کامل

Investigation of the mechanical properties and microstructure of the Ti-6Al-4V to Al2024 joint fabricated by successive- stage transient liquid phase (S-TLP) method

The aim of this study is investigation of TLP variables on microstructure and mechanical properties of Al2024 to Ti-6Al-4V bonding for TLP joint. For this purpose, the sheets were prepared with dimension of 130×32×3 mm from Ti-6Al-4V and Al2024 alloys and 50µm thick Sn-5.3Ag-4.2Bi foil as interlayer. Sn-5.3Ag-4.2Bi foil prepared with dimension of 32×25 mm. Two alloys was joint together by proce...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2017