Fracture resistance of metal ceramic restorations with two different margin designs after exposure to masticatory simulation.

نویسندگان

  • Konstantinos X Michalakis
  • Athanasios Stratos
  • Hiroshi Hirayama
  • Kiho Kang
  • Foteini Touloumi
  • Yukio Oishi
چکیده

STATEMENT OF PROBLEM Although the esthetic outcome of a collarless metal ceramic restoration is superior to that of a restoration with a metal margin, its mechanical strength has not been evaluated. PURPOSE The purpose of this study was to evaluate and compare the fracture resistance of metal ceramic restorations with metal margins to that of metal ceramic restorations with circumferential porcelain margins, after exposure to masticatory simulation. MATERIAL AND METHODS Twenty-four metal ceramic restorations were fabricated and paired with 24 cobalt-chrome tooth analogs. Twelve of the specimens had metal margins, while the remainder had circumferential porcelain margins. The restorations were cemented on the metal tooth analogs with a resin-modified glass ionomer luting agent (FujiCEM). All specimens were subjected to cyclic loading by a texture analyzer. A total of 600,000 loading cycles in an aqueous environment was performed, with a minimum load of 0 N and a maximum load of 200 N. Controlled loads were then applied to the teeth until fracture, using a stainless steel rod with a 2-mm-wide, rounded end, mounted in a universal testing machine. The specimens were examined under a stereomicroscope to determine failure mode. Descriptive statistics and the independent t test (alpha=.05) were used to determine the effect of failure loads among the tested groups. RESULTS The independent t test revealed statistically significant differences among the 2 tested groups (P<.001). The 2 groups presented different failure modes. Metal ceramic restorations with metal margins presented cohesive failures starting from the point of load application. Metal ceramic restorations with circumferential porcelain margins demonstrated a combination of adhesive and cohesive failures, starting from the point of load application and extending to the highest point of the proximal margins. CONCLUSIONS Metal ceramic restorations with metal margins required significantly greater loads (P<.001) to fracture than metal ceramic restorations with circumferential porcelain margins. (J Prosthet Dent 2009;102:172-178).

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Effect of Different Marginal Designs on the Fracture Resistance of Monolithic Zirconia Crowns

Abstract   Background and Aim: One of the major problems of all ceramic restorations is their probable fracture against the occlusal force. The aim of the present in vitro study is to compare the effect of three marginal designs (shoulder, sloped shoulder, chamfer) on the fracture resistance of monolithic zirconia crowns. Materials and methods: In this in vitro study, three PEEK dies with cham...

متن کامل

Effect of marginal design on fracture resistance of IPS e.maxall ceramic restorations: Chamfer versus shoulder finish lines

Background and Aim: One of the problems of all ceramic restorations is their risk of fracture due to occlusal loads. The aim of the present study was to compare the effect of two marginal designs (shoulder and chamfer) on the fracture resistance of IPS-emax all ceramic restorations. Materials and Methods: One extracted maxillary first premolar received chamfer 50' marginal preparation (0.8 m...

متن کامل

Mind the Crown Margins

Metal free ceramic restorations have increased in demand due to their superior esthetics and more resemblance to the natural teeth, more so now that metal-free biocompatible options are preferred. Although porcelain fused to metal crowns are also used owing to less tooth structure loss in their preparation, the metal portion shows through the marginal area giving a blue-gray, cyanotic appearanc...

متن کامل

In Vitro Evaluation of Fracture Resistance of Zirconia Restorations Veneered by Two Different Systems: Rapid Layer Technique and Zir/CAD/CAM

Background: This study aimed to assess the fracture resistance of zirconia restorations fabricated with rapid layer (RL group) technique and zirconia computer-aided design/computer-aided manufacturing (zir/CAD/CAM) system (ZC group). Methods:This study evaluated 30 all-ceramic crowns in two groups of 15. After fabricating the metal dies and scanning them ...

متن کامل

Alternate metal framework designs for the metal ceramic prosthesis to enhance the esthetics

PURPOSE The objective of the present study was to evaluate the effect of five different metal framework designs on the fracture resistance of the metal-ceramic restorations. MATERIALS AND METHODS For the purpose of this study, the central incisor tooth was prepared, and the metal analogue of it and a master die were fabricated. The counter die with the 0.5 mm clearance was used for fabricatin...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • The Journal of prosthetic dentistry

دوره 102 3  شماره 

صفحات  -

تاریخ انتشار 2009