Effect of Sandblasting Angle and Distance on Biaxial Flexural Strength of Zirconia-based Ceramics.
نویسندگان
چکیده
AIM Surface treatment is necessarily required for bonding of zirconia to the veneering porcelain and luting cements. Sandblasting is the most common and probably the most efficient surface treatment method. Sandblasting roughens the surface and may affect the flexural strength of zirconia. Different sandblasting protocols may yield variable results. This study sought to assess the effect of sandblasting angle and distance on the biaxial flexural strength of zirconia-based ceramics. MATERIALS AND METHODS This in vitro experimental study was conducted on 50 zirconia discs measuring 1.2 ± 0.2 mm in thickness and 15 ± 0.2 mm in diameter, which were randomly divided into five groups (n = 10) of one control and four experimental groups subjected to sandblasting with 110 μm aluminum oxide particles under 2 bar pressure for 10 seconds at 15 and 25 mm distances and 45 and 90° angles (between the nozzle head and zirconia surface). Surface roughness was measured by a roughness tester and samples were subjected to thermocycling followed by biaxial flexural strength testing according to ISO6872. The data were analyzed using one-way analysis of variance (p < 0.05). RESULTS No statistically significant difference was noted in the mean biaxial flexural strength of the five groups (p = 0.40). Different sandblasting protocols yielded significantly different surface roughness values (p < 0.001). The highest and the lowest mean surface roughness belonged to 15 mm/90° (0.51 μm) and control (0.001 μm) groups respectively. CONCLUSION Change in sandblasting angle and distance had no significant effect on the biaxial flexural strength of zirconia-based ceramic, but surface roughness was significantly different in the study groups. Clinical significances: Regardless of sandblasting angle, increasing distance to 25 mm significantly decreases surface roughness that may negatively affect zirconia bond strength.
منابع مشابه
Effect of Ceramic Surface Treatments After Machine Grinding on the Biaxial Flexural Strength of Different CAD/CAM Dental Ceramics.
OBJECTIVES This study aimed to evaluate the effect of different ceramic surface treatments after machining grinding on the biaxial flexural strength (BFS) of machinable dental ceramics with different crystalline phases. MATERIALS AND METHODS Disk-shape specimens (10mm in diameter and 1.3mm in thickness) of machinable ceramic cores (two silica-based and one zirconia-based ceramics) were prepar...
متن کاملبررسی اثر رنگآمیزی بر استحکام خمشی سرامیک زیرکونیایی Rainbow
Background and Aims: Along with the advances in dental materials and invention of new techniques for ceramic producion, the demand for the beauty and matching restoration’s color with patient’s natural teeth is growing. Nowadays, zirconia systems are the focus of attention. Despite their strength, one of the problems with such systems is the high opacity and failing to provide the favored col...
متن کاملPii: S0109-5641(99)00070-6
Objectives: This study was conducted to evaluate the effect of grinding and sandblasting on the microstructure, biaxial flexural strength and reliability of two yttria stabilized tetragonal zirconia (Y-TZP) ceramics. Methods: Two Y-TZP powders were used to produce fine grained and coarse grained microstructures. Sixty discs from each material were randomly divided into six groups of ten. For ea...
متن کاملFlexural strength of veneering ceramics for zirconia.
OBJECTIVES The flexural strengths of veneering ceramics for zirconia were compared. METHODS With 10 different veneering ceramics for zirconia (test group) and three different veneering ceramics for the metal-ceramic technique (control group) three-point flexural strength and biaxial flexural strength according to ISO 6872: 1995 as well as four-point flexural strength according to EN 843-1: 20...
متن کاملEffect of Thermal and Mechanical Aging on Flexural Strength of Zirkonzahn and Mamut Zirconia Ceramics
Objective: Despite the high strength of zirconia restorations, aging in the oral environment and masticatory loading may result in transformation of tetragonal to monoclinic phase and decrease their strength. Statements in this regard are controversial. This study sought to compare the flexural strength (FS) of Zirkonzahn (ZirkonZahn, Cercon, Ceramill) and Mamut (Dubai Medical Equipment LLC, ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- The journal of contemporary dental practice
دوره 18 6 شماره
صفحات -
تاریخ انتشار 2017