Influence of dentin pretreatment on bond strength of universal adhesives
نویسندگان
چکیده
Objective: The purpose of the present study was to compare bond strength of different universal adhesives under three different testing conditions: when no pretreatment was applied, after 37% phosphoric acid etching and after glycine application. Materials and methods: One hundred and fifty bovine permanent mandibular incisors were used as a substitute for human teeth. Five different universal adhesives were tested: Futurabond M+, Scotchbond Universal, Clearfil Universal Bond, G-Premio BOND, Peak Universal Bond. The adhesive systems were applied following each manufacturer's instructions. The teeth were randomly assigned to three different dentin surface pretreatments: no pretreatment agent (control), 37% phosphoric acid etching, glycine pretreatment. The specimens were placed in a universal testing machine in order to measure and compare bond strength values. Results: The Kruskal-Wallis analysis of variance and the Mann-Whitney test were applied to assess significant differences among the groups. Dentin pretreatments provided different bond strength values for the adhesives tested, while similar values were registered in groups without dentin pretreatment. Conclusions: In the present report, dentin surface pretreatment did not provide significant differences in shear bond strength values of almost all groups. Acid pretreatment lowered bond strength values of Futurabond and Peak Universal Adhesives, whereas glycine pretreatment increased bond strength values of G Praemio Bond adhesive system.
منابع مشابه
Effect of Chlorhexidine on Micro-Shear Bond Strength of Two Adhesive Systems After Aging
Background and Aim: Recurrent caries and low bond strength are the main causes of composite restorations failure. This study sought to assess the effect of chlorhexidine (CHX) on micro-shear bond strength (MSBS) to dentin of a fourth generation adhesive system and a universal bonding agent after aging. Materials and Methods: This in vitro study used 32 extracted third molars and 3-5mm thick de...
متن کاملاستحکام باند برشی سه نوع سیستم ادهزیو به مینا و عاج دندانهای دایمی
Background and Aims: The purpose of this experimental study was to investigate the shear bond strength of three new adhesive systems to enamel and dentin of permanent human teeth using three new etch and rinse and self-etch adhesive systems.Materials and Methods: Sixty intact caries-free third molars were selected and randomly divided into 6 groups. Flat buccal and lingual enamel and dentin sur...
متن کاملبررسی اثر تعداد لایههای ادهزیو بر استحکام باند ریز برشی و ریز سختی سطح باند شده عاج پس از کاربرد چهار نوع ادهزیو
Background and Aims: In this in-vitro study, the effect of multiple adhesive coating on the microshear bond strength of composite to dentin and surface microhardness of dentin after treatment with four adhesives (One Step Plus, One Step, Single Bond, Single Bond 2) were evaluated. Materials and Methods: One hundred intact human molars were cut to obtain disks of dentin having 2 mm thickness. F...
متن کاملStrength and Durability of a New Adhesive Bond to Superficial Dentin Using Etch and Rinse and Self-Etch Systems: An In Vitro Study
Background and Aim: Data regarding the efficacy of universal adhesives are limited. This study aimed to assess the durability of a universal adhesive bond to superficial dentin using etch and rinse and self-etch modes. Materials and Methods: In this in vitro, experimental study, 32 sound molars were randomly divided into two groups of Scotchbond Universal adhesive with two-step etch and rins...
متن کاملInfluence of zinc-oxide eugenol, formocresol, and ferric sulfate on bond strength of dentin adhesives to primary teeth.
This study evaluated in vitro the influence of a temporary filling {zinc oxide-eugenol (ZOE)} and two pulpotomy agents {formocresol (FC) and ferric sulfate (FS)} on shear bond strength (SBS) of two dentin adhesives to the dentin of primary molars. A total of 80 dentin surfaces were prepared and randomly allocated into 10 groups of 8 specimens each. Groups were subjected to different treatments,...