The microstructure of binary Al3Sc and ternary Al3(Sc1−yXy), where X is one of the transition metals from Group IIIA (Y), IVA (Ti, Zr or Hf) or VA (V, Nb or Ta), was investigated as a function of alloying element concentration for 0.1 y 0.75. Alloys with Group IIIA and IVA additions exhibited a single L12 solid-solution phase with some Kirkendall porosity. At the highest concentration studied, a second phase precipitated with the D019 (Y), D022 (Ti) or D023 (Zr and Hf) structure. Conversely, alloys with Group VA additions exhibited both the L12 trialuminide phase and a dendritic trialuminide second phase with D022 structure for all concentrations studied. The solubility limit in the ternary L12-type Al3(Sc1−yXy) phase was high for Group IIIA and IVA metals (almost 12.5 at.% or y=0.5), and much lower for Group VA metals (from about 1.8 at.% or y=0.07 for Ta to about 2.7 at.% or y=0.11 for V). Similarly, the solubility limit of Sc in the non-L12 phases decreases from the Group IIIA trialuminide to the Group VA trialuminides. The lattice parameter of the L12 solid-solution decreased linearly with increasing concentration of Group IVA and VA metals, but increased linearly with concentration of Y (Group IIIA). This linear concentration dependence of the lattice parameter is found to correlate with the atomic size mismatch between Sc and the transition metal. The microhardness of the L12 solid-solution increased linearly with increasing concentration of ternary elements. The concentration dependence of hardness is strongest for Group VA metals and weakest for Group IVA metals, for which a correlation is found with the concentration dependence of lattice parameter. © 2002 Elsevier Science B.V. All rights reserved.
منابع مشابه
Mechanical Properties and Microstructure of Al – Sc with Rare - Earth Element or Al 2 O 3 Additions
Mechanical Properties and Microstructure of Al–Sc with Rare-Earth Element or Al2O3 Additions Richard Albert Karnesky, Jr. Aluminum alloys strengthened with coherent (L12), nanosize Al3Sc precipitates are structural materials that have outstanding strength at ambient and elevated temperatures. They are creep resistant at 300 ◦C and exhibit a threshold stress, below which creep is not measurable....
متن کاملTHERMAL ANALYSIS AND KINETICS OF THE PRECIPITATION IN WROUGHT Al-Mg, Al-Mg-ScAND Al-Mg-Sc-Me (Me=Zr, Ti) ALLOYS
Precipitation behaviour of wrought Al-6Mg alloys with ternary scandium and quaternary zirconium and titanium has been studied. Hardness measurements and resistivity studies are employed to assess the precipitation behaviour of scandium doped Al-6Mg alloy without or with quaternary additions of zirconium and titanium. Further, the kinetics of precipitations are studied by differential scanning c...
متن کاملMicrostructure of Al3Sc with ternary rare-earth additions
The microstructure of ternary L12-Al3(Sc1 yREy) intermetallics, where RE is one of the rare-earth elements selected from five light (La, Ce, Nd, Sm or Eu) or two heavy lanthanoids (Yb or Lu), was investigated as a function of RE concentration for 0.02 y 0.75. Alloys with light RE show two phases: L12-Al3(Sc,RE) and D019-Al3(RE,Sc) (or C11b-Al4(Eu,Sc)). Alloys with heavy RE exhibit a single L12A...
متن کاملExperimental Analysis of Microstructure and Mechanical Behaviour in Fine Grained Al-Zn-Mg Alloy
The high strength Al-Zn-Mg alloy is widely used for structure components in critical aerospace applications. Small additions of scandium (Sc) often refine cast microstructure and mechanical properties by forming metastable Al3Sc dispersoids. The main role of the Al3Sc dispersoid is to prevent recrystallization during hot deformation and solution treatment. A new technique to apply for surface m...
متن کاملInfluence of shielding gas composition on weld structure in pulsed Nd: YAG laser welding
This work studied the effect of additions of carbon dioxide to argon shielding gas on the weld shape and microstructure of ST14 steel in pulsed Nd: YAG laser welding. By additions of carbon dioxide up to 15%,the weld area and depth/width ratio decreases while rising of carbon dioxide up to 25% causes increasing of weld area and depth/width ratio. It is observed that the weld metal microstructur...