Process Variations to Normally-off GaN HEMTs on Si with p-GaN Cap Layer

نویسندگان

  • Liang-Yu Su
  • Finella Lee
  • JianJang Huang
چکیده

Effects of process flows and device structures on the electrical properties of enhancement mode high electron mobility transistors (HEMTs) are investigated in this work. Except the demonstration of high threshold voltage (Vth) of 4.3V, the process window of the p-GaN residual thickness to ensure a steady operation current was estimated to be 10±5nm in our case. However, to achieve a high breakdown voltage of 1630V, a precise control of 5nm residual is required to prevent the breakdown of p-GaN take place. INTRODUCTION GaN based high electron mobility transistors (HEMTs) on silicon substrates have received much attention in power electronics due to their low-channel resistance, highbreakdown voltage, and high switching frequency. However, the inherent normally-on behavior excludes GaN based HEMTs from most power electronic applications. Among the methods proposed to achieve enhancement mode (Emode) operation, literatures on HEMTs using a p-type cap layer have reported the threshold voltage (Vth) ranging from 1V to 3V with the applied gate voltage larger than 5V [1-3]. Despite excellent performance reported, most works focused on demonstrating E-mode properties without comprehensive investigation on the correlation of the p-GaN layer structure with the electrical properties of an E-mode device, which is critical to ensure successful commercialization in the future. In this work, the E-mode HEMT operation is demonstrated by growing a heavily-doped p-GaN cap layer on an AlGaN/GaN structure. The dependence of 2DEG carrier depletion and transport mechanism on the p-GaN layer thickness was studied by different process approaches. We conclude with an E-mode GaN HEMT with a large gate voltage of 10V and a high breakdown voltage of 1630V. EXPERIMENT The epi-structure was grown on a Si (111) substrate and is composed of a 2.4μm buffer, a 1.2μm GaN, a 10nm Al0.25Ga0.75N barrier and a 60nm Mg-doped p-type GaN layer. Three process variations were employed. As Fig. 1 shows, Process A and B were designed for E-mode devices. For Process A, because the source and drain contact pads are positioned on AlGaN, the p-GaN cap layer on the source and drain was first removed by ICP-RIE before depositing the self-aligned Ti/Al/Ni/Au metal. After thermal alloy, Ni/Au metal stack was evaporated to form the schottky gate contact. Last, the p-GaN cap layer was etched to the desired thickness using the electrodes as the etching mask. For Process B, the p-GaN layer was first etched except the gate contact island. Then source and drain ohmic metal was evaporated and alloyed before schottky gate metal was deposited. To investigate the effect of p-GaN layer, Process C was performed with almost all the p-GaN cap layer etched. For all three types of processes, to prevent the etching damage to the AlGaN layer, we intentionally chose the etching depth to be either 45nm or 55nm. We design 5 devices with the nomenclature defined in Table 1. The gate– source offset length (LGS), gate length (LG), gate–drain offset length (LGD), gate width is 2, 4, 6 and 50 μm, respectively. DISCUSSION The transfer characteristic of device A45L is shown in Fig. 2 and the Vth based on the linear extrapolation gives a value of 4.3V, which is the highest among the reports on AlGaN/GaN HEMTs using Ni/Au schottky metal semiconductor contact [1-3]. Alternatively, the Vth can be estimated by the gate bias at a drain current of 1mA/mm, rendering a Vth of 4.0 V. The origin of high Vth is mainly due to the thin AlGaN structure, which also lead to a low operating current of 32mA/mm at VGS=10V. Since there typically exist 3~5nm residual p-GaN underneath the ohmic contact metal, device A45H, which adopted higher thermal alloy temperature can help to alloy through the p-GaN layer and achieve better contact resistance. The transfer characteristics show that the operation current of device A45H is 4.2 times higher than device A45L at VGS=10V, and the Vth estimated from drain current of 1mA/mm will reduce from 4V to 1.5V. The detailed analysis shows that the alloy process will affect the barrier height between gate metal and p-GN/AlGaN/GaN structure. For the devices using Process B, we further examine the dependence of electrical performance on the p-GaN residual layer with etching depths of 45 and 55nm. For comparison, Process C, which is similar to the conventional AlGaN/GaN HEMT structure, is fabricated with an etching depth of 55nm. The transfer characteristics of device C55H, B45H and B55H are shown in Fig. 3. The corresponding Vth, evaluated by the gate bias at a drain current of 1mA/mm, are -1.1, 1.6 and 1.7V, respectively. The 2.8V Vth difference between B55H and C55H indicates that the shift of Vth is related to the effect of p-GaN cap layer. Also, the transfer characteristic of device B45H is very similar to B55H, showing that the additional 10nm etching has little effect on the carrier depletion in the channel and the process window of etching depth can be estimated as 50±5nm. The breakdown measurement was carried out at the gate-source voltage of 0V due to the E-mode operation. The soft breakdown voltage at ID = 1mA/mm of device A45L, B45H and B55H with LGD = 6 μm are 257V, 448V and 566V, respectively. The gate island first (process B) process can achieve higher breakdown voltage and the 10nm additional p-GaN layer of device B45H leads to a lower breakdown voltage as compared to device B55H. To further investigate the effect of different etching depth and process conditions, Fig. 4 shows the device breakdown characteristics with respect to LGD. For Process A or B, the breakdown voltages are almost independent of LGD for the devices with the etching depth of 45nm, which means that within the LGD range of discussion, the p-GaN layers dominate the breakdown behavior. As there are less residual p-GaN layers above the channel, device B55H have the largest breakdown voltage in Fig. 4, among which a breakdown voltage as high as 1630V can be achieved with LGD=16μm. CONCLUSIONSE-mode GaN HEMTs were demonstrated with p-GaNcap layer and dependence of electrical properties on theprocess flow and device structure was investigated in thiswork. Vth can be adjusted by thermal alloy process and canextend to a value of 4.3V. The effects of p-GaN residualthickness were investigated and the process window toensure a steady current is 10±5nm in our case. However, toachieve a high breakdown voltage of 1630V, a precisecontrol of 5nm p-GaN residual thickness is required. REFERENCES[1] Y. Uemoto, et al., "Gate injection transistor (GIT)—A normally-offAlGaN/GaN power transistor using conductivity modulation," IEEE T.Electron Dev., vol. 54, pp. 3393-3399, Dec. 2007.[2] I. Hwang, et al., "1.6 kV, 2.9 mΩ cm normally-off p-GaN HEMTdevice," in Int. Sym. Pow. Semicond., June 2012, pp. 41-44.[3] O. Hilt, et al., "Normally-off high-voltage p-GaN gate GaN HFETwith carbon-doped buffer," in Int. Sym. Pow. Semicond., May 2011,pp. 239-242. Fig. 1 Illustration of three types of fabrication procedures.Fig. 2 Transfer characteristics of device A45L. The drain current isexpressed in logarithmic (left) and linear (right) scale. Fig. 3. Transfer characteristics of the device C55H, B45H and B55H Fig. 4 Breakdown voltages of the devices with various LGD. In this plot,devices fabricated using Process A and B are compared, along with 45 and55nm etch depths for Process B.TABLE I Process conditions of the devices using Process A, B and C Device Process P-GaN etching depth Alloy A45L A45nm850°C A45H A45nm900°C B45H B45nm900°C B55H B55nm900°C C55H C55nm900°C

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Normally-Off AlGaN/GaN HEMTs with InGaN cap layer: A simulation study

AlGaN/GaN high electron mobility transistors (HEMTs) are favored for the use in high-power and highfrequency applications. Normally-off operation has been desired for various applications, but proved to be difficult to achieve. Recently, a new approach was proposed by Mizutani et al. [Mizutani T, Ito M, Kishimoto S, Nakamura F. AlGaN/GaN HEMTs with thin InGaN cap layer for normally-off operatio...

متن کامل

Study of the Conduction Properties of the n GaN Cap Layer in GaN/InAlN/GaN E-HEMTs

Carrier transport in normally-off n GaN/InAlN/AlN/GaN high electron mobility transistors is studied using two-dimensional numerical device simulation. We focus on the n GaN cap layer, which is removed under the gate, and its contribution to drain current. Our simulation results show that despite the high doping density and relatively high carrier concentration in this layer, no significant tran...

متن کامل

Effects of hydrostatic pressure and temperature on the AlGaN/GaN High electron mobility transistors

In this paper, drain-source current, transconductance and cutoff frequency in AlGaN/GaN high electron mobility transistors have been investigated. In order to obtain parameters of exact AlGaN/GaN high electron mobility transistors such as electron density, the wave function, band gap, polarization charge, effective mass and dielectric constant, the hydrostatic pressure and temperature effects a...

متن کامل

On the Operation Mechanism and Device Modeling of AlGaN/GaN High Electron Mobility Transistors (HEMTs)

In this work, the physical based device model of AlGaN/GaN high electron mobility transistors (HEMTs) has been established and the corresponding device operation behavior has been investigated also by using Sentaurus TCAD from Synopsys. Advanced AlGaN/GaN hetero-structures with GaN cap layer and AlN spacer have been considered and the GaN cap layer and AlN spacer are found taking important role...

متن کامل

Breaking Through the Multi-Mesa-Channel Width Limited of Normally Off GaN HEMTs Through Modulation of the Via-Hole-Length

We present new normally off GaN high-electron-mobility transistors (HEMTs) that overcome the typical limitations in multi-mesa-channel (MMC) width through modulation of the via-hole-length to regulate the charge neutrality screen effect. We have prepared enhancement-mode (E-mode) GaN HEMTs having widths of up to 300 nm, based on an enhanced surface pinning effect. E-mode GaN HEMTs having MMC st...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2013