چکیده

The exhaust system has a number of requirements to fulfil. The major ones are to reduce the noise level created by the engine, to channel the waste gases out the rear of the automobile, to minimize the reduction in engine performance, and to have an acceptable service life and cost1. The exhaust system is divided into two main parts, the hot end and the cold end. The components comprising the hot end are the exhaust manifold, the front pipe, and the catalytic converter (if present). The cold end components include the centre pipe, the muffler, and the tail pipe. Typical operating temperatures of the different components are shown in Table I. Of all automobile exhaust failures, about 80% are caused by corrosion while the majority of the remainder are caused by fatigue1. In 1987, an Armco investigation involved the examination of nearly 350 passenger car and light truck failed exhaust systems in the Ohio area. Of the coated carbon steel failures, 70% were failures originating on the interior surface—the remaining 30% were from the exterior surface. The rate of corrosion attack originating from the exterior surface of the exhaust system is strongly influenced by the region in which the automobiles are used. The corrosivity of the external environment is far more severe in cold countries. This is due to the presence of chloride based de-icing salts that are dispersed on the roads to lower the melting point of water, and thereby reduce the amount of ice or snow on the roads. De-icers are selected on the basis that they exhibit a eutectic temperature several degrees lower than the ambient temperature encountered in the ice or snow environment. The eutectic point occurs at the salt concentration where the solution has a minimum melting temperature. For the de-icers to be feasible, they need to be comparatively cheap, must be highly soluble in water at low temperatures, External corrosion resistance of steel and ferritic stainless steel exhaust systems

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Electrochemical and passivation behavior investigation of ferritic stainless steel in simulated concrete pore media

The applications of stainless steel are one of the most reliable solutions in concrete structures to reduce chloride-induced corrosion problems and increase the structures service life, however, due to high prices of nickel, especially in many civil engineering projects, the austenitic stainless steel is replaced by the ferritic stainless steels. Compared with austenite stainless steel, the fer...

متن کامل

Evaluation of microstructure and corrosion behavior of dissimilar laser joint between Inconel 625 and AISI 430 ferritic stainless steel

Dissimilar weld joints between stainless steels and nickel based super alloys are extensively used in petrochemical, gas and oil applications. These joints jave great challenges from metallurgical transformations point of view. In this research, microstructural evolutions and corrosion behavior of laser weld joint between Inconel 625 and AISI 430 ferritic stainless steel were investigated. Ferr...

متن کامل

Thermal Fatigue Behavior of 400 Series Ferritic Stainless Steels

In this study, thermal fatigue properties of 400 series ferritic stainless steels have been evaluated in the temperature ranges of 200-800C and 200-900C. Systematic methods for control of temperatures within the predetermined range and measurement of load applied to specimens as a function of temperature during thermal cycles have been established. Thermal fatigue tests were conducted under ful...

متن کامل

An Investigation on Corrosion and Stress Corrosion Cracking initiation of a Ferritic Stainless Steel in a Tertiary Amine Solution

The present study focused on stress corrosion cracking (SCC) and corrosion behavior of ferritic stainless steel (grade 430) in activated methyl diethanolamine (aMDEA) solution, which is classified as a tertiary amine. In this regard, cyclic polarization and U-bend tests were performed in CO2 loaded aMDEA with different concentrations at 25 and 70 °C to observe corrosion behavior and ...

متن کامل

Precipitation sequence in niobium-alloyed ferritic stainless steel

Niobium is an important alloying element in the design of heat-resistant ferritic stainless steels for automotive exhaust systems. When in solid solution, it improves both the high temperature strength and the resistance to thermal fatigue. However, it also forms several kinds of precipitates during service. These reactions have been modelled, taking into account the multicomponent nature of th...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2003