The Effects of Prophylactic Ozone Pretreatment of Enamel on Shear Bond Strength of Orthodontic Brackets Bonded with Total or Self-Etch Adhesive Systems

نویسندگان

  • Sevi Burcak Cehreli
  • Asli Guzey
  • Neslihan Arhun
  • Alev Cetinsahin
  • Bahtiyar Unver
چکیده

OBJECTIVES The aim of this in vitro study is to determine (1) shear bond strength (SBS) of brackets bonded with self-etch and total-etch adhesive after ozone treatment (2) bond failure interface using a modified Adhesive Remnant Index (ARI). METHODS 52 premolars were randomly assigned into four groups (n=13) and received the following treatments: Group 1: 30 s Ozone (Biozonix, Ozonytron, Vehos Medikal, Ankara, Turkey) application + Transbond Plus Self-Etching Primer (SEP) (3M) + Transbond XT (3M), Group 2: Transbond Plus SEP + Transbond XT, Group 3: 30 s Ozone application + 37% orthophosphoric acid + Transbond XT Primer (3M) + Transbond XT, Group 4: 37% orthophosphoric acid + Transbond XT Primer + Transbond XT. All samples were stored in deionised water at 37°C for 24 hours. Shear debonding test was performed by applying a vertical force to the base of the bracket at a cross-head speed of 1 mm/min. RESULTS The mean SBS results were Group 1: 10.48 MPa; Group 2: 8.89 MPa; Group 3: 9.41 MPa; Group 4: 9.82 MPa. One-Way Variance Test revealed that the difference between the groups was not statistically significant (P=0.267). Debonded brackets were examined by an optical microscope at X16 magnification to determine the bond failure interface using a modified ARI. The results were (mean) Group 1: 2.38; Group 2: 1.31; Group 3: 3.00; Group 4: 1.92. Multiple comparisons showed that Groups 1 and 2, 2 and 3, 3 and 4 were statistically different (P=0.014, P<.001 and P=0.025). CONCLUSIONS Ozone treatment prior to bracket bonding does not affect the shear bond strength.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Comparison of shear bond strength of the stainless steel metallic brackets bonded by three bonding systems

Introduction: In orthodontic treatment, it is essential to establish a satisfactory bond between enamel and bracket. After the self-etch primers (SEPs) were introduced for the facilitation of bracket bonding in comparison to the conventional etch-and-bond system, multiple studies have been carried out on their shear bond strengths which have yielded different results. This study was aimed at co...

متن کامل

Comparing the Effect of Assure Plus and Transbond XT Bonding on Shear Bond Strength and Adhesive Remnant Index in Metal Brackets Bonded to Enamel

Background and purpose: Bracket debonding is a major problem during orthodontic treatment. This research aimed at studying shear bond strength (SBS) and adhesive remnant index (ARI) in two bonding systems (Assure Plus (adhesion booster) and control). Materials and methods: In this vitro trial, premolars (n=90) were divided into two groups. The brackets were bonded either with Transbond XT or A...

متن کامل

In vitro Effects of a Neutral Fluoride Agent on Shear Bond Strength and Microleakage of Orthodontic Brackets

Introduction: This study aimed to evaluate the effect of pretreatment with a neutral fluoride agent on shear bond strength (SBS) and microleakage of orthodontic brackets, and to investigate any significant relationship between SBS and microleakage. Methods: Forty intact premolars were selected and randomly divided into 2 groups. Group 1 served as the control, while group 2 underwent treatment w...

متن کامل

Shear bond strength and debonding characteristics of a new premixed self-etching with a reference total-etch adhesive

BACKGROUND To determine the shear bond strength and adhesive remnant index of a new premixed self-etching primer and adhesive (Tectosan, BonaDent, Germany) for orthodontic appliances in comparison to a reference total-etch system Transbond XT. METHODS Bovine incisors were embedded in resin and randomly divided into two groups of 16 samples each. Brackets (Discovery, Dentaurum, Germany) were b...

متن کامل

Effect of Saliva Contamination and sequencing time of curing the Transbond™ Plus Self Etching Primer on the Shear Bond Strength of Orthodontic Brackets

Abstract Background and aim: Over the years, improvments have been done to simplify clinical bonding procedure. One of these material is Transbond™ Plus Self Etching. The aim of this study was to evaluate the effect of saliva contamination and reusing Transbond™ Plus Self Etching Primer (SEP) on shear bond strength of orthodontic brackets. Materials and Methods: Fifty premolars divided into fiv...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 4  شماره 

صفحات  -

تاریخ انتشار 2010