Local deformation behavior of surface porous polyether-ether-ketone.

نویسندگان

  • Nathan T Evans
  • F Brennan Torstrick
  • David L Safranski
  • Robert E Guldberg
  • Ken Gall
چکیده

Surface porous polyether-ether-ketone has the ability to maintain the tensile monotonic and cyclic strength necessary for many load bearing orthopedic applications while providing a surface that facilitates bone ingrowth; however, the relevant deformation behavior of the pore architecture in response to various loading conditions is not yet fully characterized or understood. The focus of this study was to examine the compressive and wear behavior of the surface porous architecture using micro Computed Tomography (micro CT). Pore architectures of various depths (~0.5-2.5mm) and pore sizes (212-508µm) were manufactured using a melt extrusion and porogen leaching process. Compression testing revealed that the pore architecture deforms in the typical three staged linear elastic, plastic, and densification stages characteristic of porous materials. The experimental moduli and yield strengths decreased as the porosity increased but there was no difference in properties between pore sizes. The porous architecture maintained a high degree of porosity available for bone-ingrowth at all strains. Surface porous samples showed no increase in wear rate compared to injection molded samples, with slight pore densification accompanying wear.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

High-strength, surface-porous polyether-ether-ketone for load-bearing orthopedic implants.

Despite its widespread clinical use in load-bearing orthopedic implants, polyether-ether-ketone (PEEK) is often associated with poor osseointegration. In this study, a surface-porous PEEK material (PEEK-SP) was created using a melt extrusion technique. The porous layer was 399.6±63.3 μm thick and possessed a mean pore size of 279.9±31.6 μm, strut spacing of 186.8±55.5 μm, porosity of 67.3±3.1% ...

متن کامل

Quality of Kiwifruit Juice Clarifed by Modifed Poly(Ether Ether Ketone) Hollow Fiber Membranes

Poly(ether ether ketone) with cardo group-based (PEEK-WC) membranes, in hollow fber (HF) confguration, were prepared via the dry-wet spinning technique through the phase inversion process and used to clarify kiwifruit juice. The depectinised juice was processed according to a batch concentration confguration in selected operating conditions (transmembrane pressure, 1.6 ...

متن کامل

Influence of Layer Thickness and Raster Angle on the Mechanical Properties of 3D-Printed PEEK and a Comparative Mechanical Study between PEEK and ABS

Fused deposition modeling (FDM) is a rapidly growing 3D printing technology. However, printing materials are restricted to acrylonitrile butadiene styrene (ABS) or poly (lactic acid) (PLA) in most Fused deposition modeling (FDM) equipment. Here, we report on a new high-performance printing material, polyether-ether-ketone (PEEK), which could surmount these shortcomings. This paper is devoted to...

متن کامل

Mean strain effects on cyclic deformation and fatigue behavior of polyether ether ketone (PEEK)

The fatigue behavior of polyether ether ketone (PEEK) thermoplastic was investigated under uniaxial strain-controlled cyclic loading condition with various mean strains (Rε 1⁄4 0, 0.2, and 0.25). The mean stress responses of PEEK from all mean strain fatigue tests were found to be fully-relaxed. As a result, minimum mean strain effect on fatigue behavior of PEEK was observed. Fractography analy...

متن کامل

Investigation of Wear Behavior of Biopolymers for Total Knee Replacements Through Invitro Experimentation

The average life span of knee prosthesis used in Total Knee Replacement (TKR) is approximately 10 to 15 years. Literature indicates that the reasons for implant failures include wear, infection, instability, and stiffness. However, the majority of failures are due to wear and tear of the prosthesis. The most common biopolymer used in TKR  is Ultra High Molecular Weight Polyethylene (UHMWPE). Pr...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of the mechanical behavior of biomedical materials

دوره 65  شماره 

صفحات  -

تاریخ انتشار 2017