Statistical Determination of a Fretting-Induced Failure of an Electro-Deposited Coating

نویسنده

  • Kyungmok Kim
چکیده

This paper describes statistical determination of fretting-induced failure of an electro-deposited coating. A fretting test is conducted using a ball-on-flat plate configuration. During a test, a frictional force is measured, along with the relative displacement between an AISI52100 ball and a coated flat specimen. Measured data are analyzed with statistical process control tools; a frictional force versus number of fretting cycles is plotted on a control chart. On the control chart, critical number of cycles to coating failure is statistically determined. Fretted surfaces are observed after interrupting a series of fretting tests. Worn surface images and wear profiles provide that the increase on the kinetic friction coefficient after a steady-state sliding is attributed to the substrate enlarged at a contact surface. There is a good agreement between observation of worn surfaces and statistical determination for fretting-induced coating failure.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Contact Ageing Effect on Fretting Damage of an Electro-Deposited Coating against an AISI52100 Steel Ball

This article investigates the effect of contact ageing on fretting damage of an epoxy-based cathodic electro-deposited coating for use on automotive seat slide tracks (made of cold-rolled high strength steel). Static normal load was induced at the contact between the coating and an AISI52100 ball for a certain duration. It was identified that plastically deformed contact area increased logarith...

متن کامل

Evaluation and Description of Friction between an Electro-Deposited Coating and a Ceramic Ball under Fretting Condition

This article describes fretting behavior of zirconia and silicon nitride balls on an electro-deposited coating. Fretting tests are performed using a ball-on-flat configuration. The evolution of the kinetic friction coefficient is determined, along with slip ratio. Experimental results show that the steady-state friction coefficient between ceramic balls (Si₃N₄ and ZrO₂) and an electro-deposited...

متن کامل

Investigation on magnetic and microwave behavior of magnetite nanoparticles coated carbon fibers composite

Radar absorbing materials, i.e. magnetite (Fe3O4) coated carbon fibers (MCCFs) were fabricated by electro-deposition technique. Black-colored single spinel phase Fe3O4 nanoparticles was easily synthesized by hydrothermal method using reduction of a Fe (III) - Triethanolamine complex in an aqueous alkaline solution at 60-80 ◦C. Uniform and compact Fe3O4 films were fabricated on nitric acid treat...

متن کامل

Crack Behavior of the Aluminum Alloy 2024 Under Fretting Conditions

The initial stage of fretting fatigue crack growth is significantly influenced by tangential force induced by fretting action along the contact surface where a mixed-mode crack growth is involved. Fretting crack behavior of aluminum alloy 2024 was studied, taking into account the problem of contact asperities. Finite element was used for the determination of the stress field near the contact su...

متن کامل

Fretting corrosion of tin-plated contacts: Evaluation of surface characteristics

The surface characteristics of the contact zone of tin-plated copper alloy contacts subjected to fretting motion for 8000, 16,800 and 48,000 cycles under unlubricated conditions are presented. The nature of the contact zone, at the verge of wearing out of the tin coating as well as upon the coating is completely worn out, is assessed using scanning electron microscopy (SEM), energy-dispersive X...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2017