In vitro and in vivo characterization of novel biodegradable polymers for application as drug-eluting stent coatings.

نویسندگان

  • Nathan A Lockwood
  • Robert W Hergenrother
  • Laura M Patrick
  • Sean M Stucke
  • Rob Steendam
  • Erica Pacheco
  • Renu Virmani
  • Frank D Kolodgie
  • Brad Hubbard
چکیده

We have used a series of in vitro and in vivo tests to assess the suitability of two new degradable polymers for application as coatings for drug-eluting stents. The first is a family of urethane-linked multi-block copolymers (MBCP) that comprise blocks of lactide, glycolide, epsilon-caprolactone and/or poly(ethylene glycol) chain-extended with 1,4-butanediisocyanate (SynBiosys polymers). The second is a family of maltodextrin (MD) modified with fatty acid sidechains to yield a hydrophobic polymer (Eureka() SOLO polymers). We coated stainless-steel stents with two representative urethane-linked MBCPs and one hydrophobic MD polymer alone or in combination with the anti-restenotic drug sirolimus. Urethane-linked MBCPs formed uniform coatings on the stent substrates, withstood crimping and expansion on balloon catheters, completely released sirolimus from the coating within 30 days, and degraded within 30-60 days in PBS. The hydrophobic MD polymer formed uniform coatings, exhibited somewhat slower release of sirolimus (approx. 85% within 30 days), degraded within 60 days in PBS when sirolimus was incorporated in the coating, but showed very slow degradation in the absence of drug. We implanted stents coated with urethane-linked MBCPs or hydrophobic MD polymers in a porcine coronary artery model and used histological analysis at 28- and 90-day end-points to assess the biological response to the materials. Measures of stenosis and inflammation for urethane-linked MBCP and hydrophobic MD polymer coatings were not statistically different from bare metal controls at 28 and 90 days, suggesting that the polymers show good vascular biocompatibility. Endothelialization was nearly complete at 28 days and complete at 90 days for all formulations. Urethane-linked MBCP polymer-only and drug-eluting coatings and hydrophobic MD drug-eluting coatings were nearly completely degraded within 90 days in vivo whereas roughly half of hydrophobic MD polymer-only coatings remained after 90 days. Taken together, our in vitro and in vivo results suggest that SynBiosys urethane-linked MBCP and Eureka SOLO hydrophobic MD polymer families possess the physical and chemical properties and vascular biocompatibility necessary for further investigation for use in the next generation of drug-eluting stents.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Advances in Interventional Cardiology New Drug-Eluting Stents An Overview on Biodegradable and Polymer-Free Next-Generation Stent Systems

Drug-eluting stents (DES)were primarily conceived to reduce in-stent neointimal formation and therefore minimize the occurrence of restenosis, the major drawback of percutaneous coronary interventions with bare-metal stents (BMS). The development of DES has been pioneered through a combination of the increased understanding of the biology of restenosis, the selection of drugs that target 1 or m...

متن کامل

New drug-eluting stents: an overview on biodegradable and polymer-free next-generation stent systems.

Drug-eluting stents (DES)were primarily conceived to reduce in-stent neointimal formation and therefore minimize the occurrence of restenosis, the major drawback of percutaneous coronary interventions with bare-metal stents (BMS). The development of DES has been pioneered through a combination of the increased understanding of the biology of restenosis, the selection of drugs that target 1 or m...

متن کامل

Scanning electron microscopic assessment of the biodegradable coating on expanded biolimus-eluting stents.

AIMS Biodegradable coatings on drug-eluting stents (DES) may help to avoid adverse long-term effects of DES such as late/very late stent thrombosis which is partly attributed to durable polymers. As the post-expansion morphology of biodegradable coatings is greatly unknown, we investigated the polylactic acid coating on biolimus-eluting BioMatrix stents. METHODS AND RESULTS Scanning electron ...

متن کامل

In vivo evaluation of biocompatible intravascular stents coated by inkjet printing

Inkjet–printing technology was used to apply biodegradable and biocompatible polymeric coatings of poly(D, L lactide) with the antiproliferative drugs simvastatin (SMV) and paclitaxel (PCX) on coronary metal stents. A piezoelectric dispenser applied coating patterns of very fine droplets (300 xL) and ink jetting was optimized to develop uniform, accurate and reproducible coatings of high yields...

متن کامل

Acute Thrombogenicity of a Durable Polymer Everolimus-Eluting Stent Relative to Contemporary Drug-Eluting Stents With Biodegradable Polymer Coatings Assessed Ex Vivo in a Swine Shunt Model.

OBJECTIVES This study sought to evaluate whether the permanent fluoropolymer-coated Xience Xpedition everolimus-eluting stent (Xience-EES) exhibits lower acute thrombogenicity compared with contemporary drug-eluting stents (DES) with biodegradable polymer coatings in an acute swine shunt model. BACKGROUND Previous pre-clinical and clinical experience suggests that several factors may influenc...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of biomaterials science. Polymer edition

دوره 21 4  شماره 

صفحات  -

تاریخ انتشار 2010