Effects of a convenient silica-coating treatment on shear bond strengths of porcelain
نویسندگان
چکیده
Significant progress has been achieved in ceramics since the late 1990s1-4). In particular, new technological innovations such as heat-pressed5,6), injection-molded7), slip-cast8), and glass-infiltrated ceramics9-11) have widened the use of ceramics in prosthetic and operative dentistry. However, properties such as brittleness limit their use in applications such as fixed partial dentures. Since the beginning of the 21st century, zirconium dioxide (ZrO2: zirconia), a new and tough ceramic material, has been receiving increasing attention in dentistry12-16). Initially, its use was restricted to metalfree fixed partial anterior dentures, but its use is being extended to a variety of applications, such as fixed partial posterior dentures, orthodontic brackets19) and dental implant abutment or fixture20,21), as well as simple dental restoration or prostheses17,18). Above all, frameworks using zirconia-based ceramics have gained popularity for use as metal-free, long-lasting, and extensive fixed dental prostheses. Zirconia-based ceramics are characterized by a tetragonal phase, a monoclinic phase, and a cubic phase, and these phases are mutually interchangeable under some kinds of stress such as heating, sandblasting, and mechanical grinding. It is also well known that volume changes occur when going from monoclinic to tetragonal crystals under the specific actions mentioned above22,23). This phase change is useful for controlling crack propagation in zirconia-based ceramics and contributes to their high fracture toughness. Formation of the tetragonal phase strongly stabilizes zirconia-based ceramics, but other crystal phases are undesirable. To maintain the tetragonal phase at room temperature, zirconia-based ceramics must be stabilized by adding oxides. Yttria is a popular stabilizing additive, giving Y-TZP12,13,16). This new ceramic is useful as a prosthetic frame material because of its high fracture toughness and its precision fabrication with dental CAD/CAM systems. A final prosthetic process is needed to deposit a porcelain veneer on zirconia-based ceramics; however, chipping of the porcelain veneer causes clinical problems. Hydrothermal degradation of the veneer with lowtemperature aging is also controversial16,24). To overcome these problems, some modification techniques have been proposed. The latest zirconia-based ceramics materials, stabilized by ceria, were developed to achieve better mechanical properties than those of Y-TZP25-28). Ceriastabilized tetragonal zirconia/alumina nanocomposites (zirconia nanocomposites) are significantly reinforced by dispersing different nanosized particles into each crystal grain. Furthermore, preparation, prior to veneering, of frameworks as thin as those of traditional porcelainfused metal (PFM) is possible because of the flexibility of these nanocomposites, so extremely light frames of thickness 0.3 mm can be obtained. In esthetic restoration, dental PFM has served the profession well for nearly a half-century, but there are many disadvantages to using metals, such as allergic reactions as a result of the release of harmful ions into the body and/or low durability. Most dentists prefer allceramic restoration to traditional PFM methods when attempting to achieve the optimum esthetic results. Generally speaking, fixed-type all-ceramic prostheses usually give better esthetic results than PFM because of the difficulty in blocking out the color and opacity of the metal substructure. Moreover, it has been reported that Effects of a convenient silica-coating treatment on shear bond strengths of porcelain veneers on zirconia-based ceramics
منابع مشابه
Low-Fusing Porcelain Glaze Application on 3Y-TZP Surfaces can Enhance Zirconia-Porcelain Adhesion.
The aim of this study was to assess whether surface treatment improves zirconia-porcelain adhesion. The 3Y-TZP blocks were cut into squares, then polished and sintered. The zirconia surface treatments were performed as follows: no treatment (C); tribochemical silica coating (TBS); glaze application + hydrofluoric acid etching (GA); glaze application + hydrofluoric acid etching + silanization (G...
متن کاملEvaluation of resin bond strength to yttria-stabilized tetragonal zirconia and framework marginal fit: comparison of different surface conditionings.
The purpose of this study was to evaluate the effect of different surface treatments of yttria-stabilized tetragonal zirconia (Y-TZP) on bond strength durability and marginal discrepancies. For adhesion testing, 144 specimens of VITA In-Ceram YZ ceramic for InLab were obtained (5.25×3.75×4.5 mm) and divided into six groups (n=24) according to the surface treatment: 1) Control (CRTL): untreated;...
متن کاملSol–gel dip coating of yttria-stabilized tetragonal zirconia dental ceramic by aluminosilicate nanocomposite as a novel technique to improve the bonding of veneering porcelain
The aim of this in vitro study was to evaluate the effect of silica and aluminosilicate nanocomposite coating of zirconia-based dental ceramic by a sol-gel dip-coating technique on the bond strength of veneering porcelain to the yttria-stabilized tetragonal zirconia polycrystal (Y-TZP) in vitro. Thirty Y-TZP blocks (10 mm ×10 mm ×3 mm) were prepared and were assigned to four experimental groups...
متن کاملComparison of the Effect of Three methods of Porcelain Surface Treatment on Shear Bond Strength of Composite to Porcelain
Background and Aim: Several methods are available for intraoral repair of chipped porcelain restorations by composite resin. Also, there is still controversy regarding the best method of porcelain repair in terms of bond strength and cost effectiveness. This study aimed to compare three methods of porcelain surface treatment on shear bond strength (SBS) of composite to porcelain. Materials a...
متن کاملIn vitro experimental study of bonding between aluminium oxide ceramics and resin cements.
UNLABELLED To evaluate bond strengths of different resin cements to two aluminum oxide-based ceramics. METHODS One hundred ten ceramic cylinders were produced and given four different surface treatments. Resin cement cylinders were then bonded to the ceramic cylinders using different resin cements and the bond strength was determined by shear testing to the breaking point. We were thus able t...
متن کامل