Leucite content of selected dental porcelains.

نویسندگان

  • P W Piché
  • W J O'Brien
  • C L Groh
  • K M Boenke
چکیده

Leucite is a major crystalline component of dental porcelains. The presence of tetragonal leucite in dental porcelains increases their coefficients of thermal expansion due to its high coefficient of thermal expansion (20-25 x 10(-6)/degrees C). This is particularly useful for those porcelains designed for bonding to precious metals and nickel alloys. The purpose of this study was to determine the leucite content of selected commercial dental porcelains in relation to their coefficient of thermal expansion values. The weight fraction of leucite was determined with quantitative x-ray diffraction using copper as an internal standard. Coefficient of thermal expansion values were determined using a thermal dilatometric analyzer. Five commercial body porcelains were studied. Leucite was not detected in samples of Vitadur N and Duceram LFC. An ANOVA showed that there was a significant difference in the weight fraction of leucite for Silhouette, Ceramco II, and Optec HSP porcelains. Linear regression revealed a correlation (R = 0.91) between weight fraction of leucite and the coefficient of thermal expansion for those samples containing leucite. Duceram LFC, which is recommended by the manufacturer for use with metals and leucite-containing porcelains, had no detectable leucite although the coefficient of thermal expansion was found to be 13.2 +/- 0.4 x 10(-6)/degrees C at 25-472 degrees C. A low glass transition temperature contributed to the high average coefficient of thermal expansion value.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Investigation on the Tribological Behavior and Wear Mechanism of Five Different Veneering Porcelains

OBJECTIVES The primary aim of this research was to investigate the wear behavior and wear mechanism of five different veneering porcelains. METHODS Five kinds of veneering porcelains were selected in this research. The surface microhardness of all the samples was measured with a microhardness tester. Wear tests were performed on a ball-on-flat PLINT fretting wear machine, with lubrication of ...

متن کامل

Effect of leucite crystals on the strength of glassy porcelain.

Porcelains with leucite crystals dispersed into various glass matrices were prepared for investigating the effects of the leucite crystals on the mechanical strength of glassy porcelain. The strength of glassy porcelains containing leucite crystals was affected by the differences of thermal expansion coefficients, compositions and deformation temperatures of the glass matrices. In the case of a...

متن کامل

Effect of cooling condition on leucite crystals in dental porcelains.

X-ray diffractometry (XRD) was used to analyze the crystal phases of three commercial dentin and incisal porcelains prepared by normal cooling, quenching in water, and controlled slow annealing after normal firing. There were no remarkable differences in the contents of either tetragonal and cubic leucite in the fired porcelain discs prepared under the three cooling conditions. Furthermore, the...

متن کامل

The effect of cesium-containing leucite additions on the thermal and mechanical properties of two leucite-based porcelains.

It has been demonstrated that a Cs(2)O-stabilized leucite porcelain was susceptible to a stress-induced phase transformation, but toughening was not observed.1 It was hypothesized that if Cs(2)O-stabilized leucite core particles were added to a cesium-free matrix porcelain, selected or designed to enhance the toughening mechanism, toughening would occur. A commercial porcelain (VP) and a synthe...

متن کامل

Flexural strength of fluorapatite-leucite and fluorapatite porcelains exposed to erosive agents in cyclic immersion

OBJECTIVE The aim of this study was to evaluate the flexural strength of two porcelain materials (IPS d.SIGN and IPS e.max Ceram) exposed to erosive agents. MATERIAL AND METHODS One hundred and twenty bar-shaped specimens were made from each of fluorapatite-leucite porcelain (IPS d.SIGN) and fluorapatite porcelain (IPS e.max Ceram) and divided into 8 groups of 15 specimens each. Six groups we...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of biomedical materials research

دوره 28 5  شماره 

صفحات  -

تاریخ انتشار 1994