Surfaces of carbon steel (CS) exposed to mixed cultures of iron-oxidizing bacteria (FeOB) and dissimilatory iron-reducing bacteria (FeRB) in seawater media under aerobic conditions were rougher than surfaces of CS exposed to pure cultures of either type of microorganism. The roughened surface, demonstrated by profilometry, is an indication of loss of metal from the surface. In the presence of CS, aerobically grown FeOB produced tight, twisted helical stalks encrusted with iron oxides. When CS was exposed anaerobically in the presence of FeRB, some surface oxides were removed. However, when the same FeOB and FeRB were grown together in an aerobic medium, FeOB stalks were less encrusted with iron oxides and appeared less tightly coiled. These observations suggest that iron oxides on the stalks were reduced and solubilized by the FeRB. Roughened surfaces of CS and denuded stalks were replicated with culture combinations of different species of FeOB and FeRB under three experimental conditions. Measurements of electrochemical polarization resistance established different rates of corrosion of CS in aerobic and anaerobic media, but could not differentiate rate differences between sterile controls and inoculated exposures for a given bulk concentration of dissolved oxygen. Similarly, total iron in the electrolyte could not be used to differentiate treatments. The experiments demonstrate the potential for iron cycling (oxidation and reduction) on corroding CS in aerobic seawater media.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The subtle effects of iron-containing metal surfaces on the reductive carbonylation of RuCl3.

The use of iron-containing metal surfaces, Fe, Fe-Cr-alloy and stainless steel, for the synthesis of mixed metal Ru-Fe compounds has been studied. The studied process was reductive carbonylation of RuCl3 in the presence of a metal surface. Reactions were carried out in ethanol solutions under 10-50 bar carbon monoxide pressure at 125 degrees C using an autoclave. During the reaction the metal s...

متن کامل

Investigation of Wear Mechanism in Quenched and Tempered Medium Carbon-High Chromium Martensitic Steel Using Dry Sand/Rubber Wheel

The aim of the present study was to investigate the effect of quenching and tempering temperatures on the microstructure, mechanical properties and the wear characteristics of medium carbon-high chromium wear resistant steel. In addition, the dominant wear mechanisms were studied. For this purpose, austenitizing and tempering temperatures were selected in the ranges of 900- 1000 °C and 300- 500...

متن کامل

Effects of alloying on the chemistry of CO and H2S on Fe surfaces.

Deleterious gases such as CO and H(2)S can cause degradation of steel by reacting with the metal surface. Here we consider whether alloying the steel surface might be able to inhibit these damaging surface reactions by raising the barriers to molecular dissociation. We employ first-principles density functional theory techniques to investigate the elementary reaction pathways and barriers for C...

متن کامل

Development of an electrochemically integrated SR-GIXRD flow cell to study FeCO3 formation kinetics.

An electrochemically integrated Synchrotron Radiation-Grazing Incidence X-Ray Diffraction (SR-GIXRD) flow cell for studying corrosion product formation on carbon steel in carbon dioxide (CO2)-containing brines typical of oil and gas production has been developed. The system is capable of generating flow velocities of up to 2 m/s at temperatures in excess of 80 °C during SR-GIXRD measurements of...

متن کامل

Developing Very Fine Nanopearlitic Structure in a High Carbon Steel Wire before Drawing

The effects of steel wire patenting process parameters on very fine interlamellar spacing in the pearlitic steel wire were investigated and the optimized condition of the process was achieved. In this work, the initial nanopearlitic structure was obtained in a 0.72 wt% carbon steel wire before the wire drawing process. The results were the minimum interlamellar spacing of 35 nm and maximum ulti...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 29  شماره 

صفحات  -

تاریخ انتشار 2013