Strength and fracture pattern of monolithic CAD/CAM-generated posterior crowns.

نویسندگان

  • Andreas Bindl
  • Heinz Lüthy
  • Werner H Mörmann
چکیده

OBJECTIVES This study evaluated the strength and fracture pattern of monolithic posterior CAD/CAM crowns hypothesizing that zinc-phosphate cemented lithium disilicate crowns might show the same fracture strength as adhesively cemented crowns. METHODS Two sets of monolithic posterior crowns each with uniform occlusal and lateral wall thickness of 1.5mm were fabricated from three types of block ceramic (1) lithium disilicate glass, (2) leucite glass and (3) feldspathic ceramic using CEREC 3 CAD/CAM. Crowns (n = 15) of ceramics (1), (2) and (3) each were (A) zinc-phosphate cemented, (B) adhesively cemented on resin-based composite dies and loaded until fracture. Load data was analyzed using ANOVA and Scheffé tests. Crack pattern was evaluated on an additional three sample cross-sections for each group at start of fracture. RESULTS Radial cracks originated early at the cementation interfaces and cone cracks were observed finally at the loading sites. Mean load values (SD) of A-crowns at fracture start/end (1) 807 (91) N/2082 (192) N; (2) 915 (193) N/1130 (166) N; (3) 985 (199) N/1270 (301) N were all significantly (P < 0.001) lower when compared to their B-crown analogs (1) 1456 (205) N/2389 (84) N; (2) 1684 (395) N/2469 (171) N; (3) 1548 (304) N/2392 (75) N, rejecting the authors hypothesis. A-1 crowns had significantly (P < 0.001) higher fracture load than A-2 and A-3 crowns. The A-1 crown fracture load data, even if significantly (P < 0.001) lower, came close to the B-1 values. SIGNIFICANCE Adhesive cementation balanced the strength of weak ceramics with that of strong ceramic and recommended itself for leucite glass ceramic and feldspathic ceramic crowns. Zinc-phosphate cementation appeared feasible for lithium disilicate crowns.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Die Materials on the Fracture Resistance of CAD/CAM Monolithic Crown Restorations

The effect of the die materials on the fracture strength of CAD/CAM monolithic ceramic crowns was studied in this research. Three different types of die materials (dentin, Ni-Cr alloy, epoxy resin) were prepared. The monolithic crowns were fabricated using a CAD/CAM System; CEREC 4. The CAD/CAM crowns were cemented to dies using a resin cement. The specimens were tested under compressive load a...

متن کامل

Fracture Strength of Aged Monolithic and Bilayer Zirconia-Based Crowns

The purpose of this study was to evaluate the effect of design and surface finishing on fracture strength of yttria-tetragonal zirconia polycrystal (Y-TZP) crowns in monolithic (1.5 mm thickness) and bilayer (0.8 mm zirconia coping and 0.7 mm porcelain veneer) configuration after artificial aging. Bovine incisors received crown preparation and Y-TZP crowns were manufactured using CAD/CAM techni...

متن کامل

Monolithic CAD/CAM lithium disilicate versus veneered Y-TZP crowns: comparison of failure modes and reliability after fatigue.

PURPOSE The aim of this research was to evaluate the fatigue behavior and reliability of monolithic computer-aided design/computer-assisted manufacture (CAD/CAM) lithium disilicate and hand-layer-veneered zirconia all-ceramic crowns. MATERIALS AND METHODS A CAD-based mandibular molar crown preparation, fabricated using rapid prototyping, served as the master die. Fully anatomically shaped mon...

متن کامل

Effect of cements on fracture resistance of monolithic zirconia crowns

Objectives The present study investigated the effect of cements on fracture resistance of monolithic zirconia crowns in relation to their compressive strength. Materials and methods Four different cements were tested: zinc phosphate cement (ZPC), glass-ionomer cement (GIC), self-adhesive resin-based cement (SRC) and resin-based cement (RC). RC was used in both dual cure mode (RC-D) and chemical...

متن کامل

Comparative fracture strength analysis of Lava and Digident CAD/CAM zirconia ceramic crowns

PURPOSE All-ceramic crowns are subject to fracture during function. To minimize this common clinical complication, zirconium oxide has been used as the framework for all-ceramic crowns. The aim of this study was to compare the fracture strengths of two computer-aided design/computer-aided manufacturing (CAD/CAM) zirconia crown systems: Lava and Digident. MATERIALS AND METHODS Twenty Lava CAD/...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Dental materials : official publication of the Academy of Dental Materials

دوره 22 1  شماره 

صفحات  -

تاریخ انتشار 2006